MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aluminum Bronze, UNS C95500, Casting Alloy, As-Cast
Categories: Metal; Nonferrous Metal; Copper Alloy; Bronze; Copper Casting Alloy

Material Notes: High strength, heat treatable.

Recommended Casting Methods: Centrifugal, Continuous, Permanent Mold, Plaster, and Sand.

Applications: Valve guides and seats in aircraft engines, corrosion-resistant parts, bushings, gears, worms, pickling hooks and baskets, agitators.

Classified under: Aluminum bronzes. ASTM B148; formerly ASTM B148-9D

Key Words: Nickel aluminum bronze, ASTM B148, ASTM B148-9D
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 7.53 g/cc0.272 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 183 - 192183 - 1923000 kg load
Hardness, Rockwell B 8787
Tensile Strength, Ultimate 620 - 710 MPa89900 - 103000 psi
Tensile Strength, Yield 275 - 310 MPa39900 - 45000 psi
Elongation at Break 6.0 - 14 %6.0 - 14 %in 50 mm
Reduction of Area 7.0 %7.0 %
Creep Strength  17.0 MPa
@Temperature 425 °C
2470 psi
@Temperature 797 °F
for 0.00001%/h
 38.0 MPa
@Temperature 370 °C
5510 psi
@Temperature 698 °F
for 0.00001%/h
 72.0 MPa
@Temperature 315 °C
10400 psi
@Temperature 599 °F
for 0.00001%/h
Modulus of Elasticity 110 GPa16000 ksi
Compressive Yield Strength 825 MPa120000 psiat permanent set of 10%
Compressive Strength 895 MPa130000 psi
Poissons Ratio 0.320.32
Fatigue Strength 215 MPa
@# of Cycles 1.00e+8
31200 psi
@# of Cycles 1.00e+8
rotating beam
Machinability 50 %50 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 42.0 GPa6090 ksi
Izod Impact 18.0 J
@Temperature 20.0 °C
13.3 ft-lb
@Temperature 68.0 °F
Charpy Impact 14.0 J10.3 ft-lbKeyhole
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000203 ohm-cm
@Temperature 20.0 °C
0.0000203 ohm-cm
@Temperature 68.0 °F
Magnetic Permeability 1.31.316 kA/m field strength
 
Thermal PropertiesMetricEnglishComments
CTE, linear 16.2 µm/m-°C
@Temperature 20.0 - 300 °C
9.00 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.418 J/g-°C0.0999 BTU/lb-°F
Thermal Conductivity 42.0 W/m-K
@Temperature 20.0 °C
291 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
Melting Point 1040 - 1055 °C1900 - 1931 °F
Solidus 1040 °C1900 °F
Liquidus 1055 °C1931 °F
Shrinkage 1.6 %1.6 %Patternmaker's Shrinkage (3/16 in./ft.)
 
Processing PropertiesMetricEnglishComments
Annealing Temperature 620 - 705 °C1150 - 1300 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 10 - 11.5 %10 - 11.5 %
Copper, Cu >= 78 %>= 78 %
Iron, Fe 3.0 - 5.0 %3.0 - 5.0 %
Manganese, Mn <= 3.5 %<= 3.5 %
Nickel, Ni 3.0 - 5.5 %3.0 - 5.5 %
Other, total <= 0.50 %<= 0.50 %
 
Descriptive Properties
Elastic Limit310 MPaas cast
 415 MPaTQ50 temper

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Alpha Nickel-Aluminum Bronze, UNS C95800, Copper Casting Alloy
Aluminum Bronze, UNS C95400, Copper Casting Alloy, As Cast
Aluminum Bronze, UNS C95200, Copper Casting Alloy
Aluminum Bronze, UNS C95500 Casting Alloy, TQ50 Temper
Nickel Aluminum Bronze, UNS C63000, Annealed Rod

MC95500b1 / 11965

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.