MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kraton® D1102 K (SBS) Liner Block Copolymer
Categories: Polymer; Thermoplastic; Styrene-Butadiene; Styrene/Butadiene/Styrene (SBS)

Material Notes: Description: Kraton D1102 K is a clear, linear triblock copolymer based on styrene and butadiene, with a polystyrene content of 28%. It is supplied from North America in the physical form identified:
Kraton D1102 KT - supplied as a dusted porous pellet
Kraton D1102 KU - supplied as an undusted porous pellet

Region: Europe, South America, Asia Pacific, Japan, and North America

Uses: Kraton D1102 K is used as a modifier of bitumen or thermoplastics and in compound formulations. It is also suitable as an ingredient in formulating compounds for footwear applications and may be used in formulating adhesives, sealants and coatings.

Applications: Adhesives, Sealant and Coatings; Bitumen Modification; Compounding and Personal Hygiene; Footwear; Impact Modification; Medical; Packaging and Polymod; Personal Care; and Roads and Roofing

Information provided by Kraton®

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.940 g/cc0.940 g/ccASTM D4025
Bulk Density 0.449 g/cc0.0162 lb/in³
Volatiles <= 0.70 %<= 0.70 %KM 04
Viscosity 1100 cP1100 cP25% Toluene Solution at 25°C; BAM 922
Melt Flow 14 g/10 min
@Load 5.00 kg,
Temperature 200 °C
14 g/10 min
@Load 11.0 lb,
Temperature 392 °F
Ash 0.20 - 0.40 %0.20 - 0.40 %Talc; BAM 908
 
Chemical PropertiesMetricEnglishComments
Diblock Content 17 %17 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 66
@Time 10.0 sec
66
@Time 0.00278 hour
Typical values on polymer compression molded at 300°F; ASTM D2240
Tensile Strength 31.7 MPa4600 psimeasured on films cast from a solution in toluene; ASTM D412
Elongation at Break 880 %880 %Measured on films cast from a solution in toluene; ASTM D412
300% Modulus 2.76 MPa
@Strain 300 %
400 psi
@Strain 300 %
film cast from poluene solution; ISO 37
 
Descriptive Properties
ContentNon-staining phenolic antioxidant0.15-0.25%, KM 08
 Polystyrene28-30%, KM 03
 Total Extractables<1.0%, KM 05
Styrene/Rubber Ratio28/72

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Kraton® D1102 E (SBS) Liner Block Copolymer
Kraton® D1102 B (SBS) Liner Block Copolymer
Kraton® FG1901 + PA-6 blend (20/80)
Kraton® FG1901 + PBT blend (30/70)
Kraton® D1102 J (SBS) Liner Block Copolymer

PKRA9812 / 132711

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.