MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboWeld 8505-1 A/B Silver-Filled Electrically Conductive Epoxy Compound
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy, Electrically Conductive

Material Notes: AboWeld 8505-1 A/B is a solventless silver-epoxy adhesive and resurfacer. It has high rigidity, chemical and heat resistance. It also has good adhesion to most rigid materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Solids Content 100 %100 %
 
Electrical PropertiesMetricEnglishComments
Surface Resistivity per Square <= 0.010 ohm<= 0.010 ohm
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 120 °C248 °F
 
Processing PropertiesMetricEnglishComments
Cure Time  30.0 - 180 min
@Temperature 50.0 - 100 °C
0.500 - 3.00 hour
@Temperature 122 - 212 °F
Optional
 >= 1440 min
@Temperature 22.0 - 30.0 °C
>= 24.0 hour
@Temperature 71.6 - 86.0 °F
Pot Life 45 min45 min
 
Descriptive Properties
ColorGray
Metal (%)75of vehicle
Parts by Weight (pbw)100Part A Resin
 2.6Part B Hardener
ViscosityPaste

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Abatron AboCoat 8401-1 A/B Silver-Filled Electrically Conductive Epoxy Compound
Latitude Manufacturing PowderFlo® 316L Stainless Steel Metal Injection Molding Compound
Aremco Aremco-Bond™ 525 Electrically & Thermally Conductive Material, Silver Filled
CHT Group EP Primer 28 EPI Engineered Polymers Aromatic polyisocyanate Prepolymer
Overview of materials for Epoxy Molding Compound

PABC846 / 107830

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.