MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

California Fine Wire Nickel Alloy 180 Copper Nickel Resistance Wire
Categories: Metal; Electronic/Magnetic Alloy; Nonferrous Metal; Copper Alloy

Material Notes: All values may vary dependent on specific design and usage

Capabilities:

  • Wire
  • Ribbon
  • Square
  • Insulated
  • Plated

Information provided by California Fine Wire.

Key Words: ASTM B267
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 345 MPa50000 psiAnnealed
 689 MPa100000 psiHard
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000299 ohm-cm0.0000299 ohm-cm3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
 
Thermal PropertiesMetricEnglishComments
CTE, linear 15.8 µm/m-°C
@Temperature 20.0 °C
8.78 µin/in-°F
@Temperature 68.0 °F
Specific Heat Capacity 0.385 J/g-°C
@Temperature 20.0 °C
0.0920 BTU/lb-°F
@Temperature 68.0 °F
Thermal Conductivity 35.0 W/m-K243 BTU-in/hr-ft²-°F
Melting Point 1100 °C2012 °F
Maximum Service Temperature, Air 1000 °C1830 °FOperating Temperature
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 78 %78 %
Nickel, Ni 22 %22 %
 
Descriptive Properties
MagneticNone
Temperature Coefficient of Resistance0.00018 ohms/ohm-°C0-100°C
Thermal EMF vs. Copper-0.037

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Copper nickel 30%, UNS C71500
Alloy Wire International RW 80 Ni-Cr Resistance Wire
Carlson 70 30 Cu Ni Copper-Nickel Alloy
Copper nickel 10%, UNS C70600
Resistor Alloy 30

NCALZ23 / 15566

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.