MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Mocom (ALBIS) ALFATER® XL A65I 2GP0000 PP/EPDM
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Base Polymer: Thermoplastic Vulcanisate PP/EPDM-Elastomer

Special Features: Good weathering resistance, resistant to alkalis, resistant to ozone, resistant to hot air, hydrolysis resistant

Market Segment: Automotive, Building and Construction, Electrical and Electronic, household goods, Sports and Leisure

Application Area: Injection molded parts

Typical Applications: Seals, handles, racking/shelving, impact protection/shock absorber, protection cap

Information provided by Albis Plastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.025 - 0.029 cm/cm
@Time 86400 sec
0.025 - 0.029 in/in
@Time 24.0 hour
ISO 294-4
Linear Mold Shrinkage, Transverse 0.013 - 0.017 cm/cm
@Time 86400 sec
0.013 - 0.017 in/in
@Time 24.0 hour
ISO 294-4
Spiral Flow 80.0 cm
@Thickness 2.00 mm
31.5 in
@Thickness 0.0787 in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 65
@Time 15.0 sec
65
@Time 0.00417 hour
ISO 868
Tensile Strength 6.80 MPa986 psitype 2; ISO 37
Tensile Stress at Strain 2.70 MPa
@Strain 100 %
392 psi
@Strain 100 %
type 2; ISO 37
Elongation at Break 375 %375 %type 2; ISO 37
Tear Strength 26.0 kN/m148 plimethod Ba; ISO 34-1
Compression Set  20 %
@Temperature 22.0 °C,
Time 259000 sec
20 %
@Temperature 71.6 °F,
Time 72.0 hour
25%, Type A; ISO 815
 35 %
@Temperature 70.0 °C,
Time 79200 sec
35 %
@Temperature 158 °F,
Time 22.0 hour
25%, Type A; ISO 815
 35 %
@Temperature 100 °C,
Time 79200 sec
35 %
@Temperature 212 °F,
Time 22.0 hour
25%, Type A; ISO 815
 50 %
@Temperature 125 °C,
Time 259000 sec
50 %
@Temperature 257 °F,
Time 72.0 hour
25%, Type A; ISO 815
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Melt Temperature 195 - 215 °C383 - 419 °FInjection molding
Mold Temperature 10.0 - 70.0 °C50.0 - 158 °FInjection molding
Drying Temperature 70.0 - 80.0 °C
@Time 7200 - 14400 sec
158 - 176 °F
@Time 2.00 - 4.00 hour
in a dry air (desiccant) dryer
 
Descriptive Properties
Base PolymerThermoplastic Vulcanizate PP/EPDM-Elastomer

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ZEON HyTemp® SC-75 Polyacrylate Curative
Monmouth Rubber & Plastics Durafoam™ P391SHD EPDM
Chemours Viton® A-700 with 3 phr Curative and 6 phr Ca(OH)2
ATG s.r.l. EPDM Ethylene-Propylene Terpolymer

PALBIS8217 / 242276

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.