MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SPS Guang Zhou REMAK™ 7001RM4 Flame-retarded PS masterbatch
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Flame Retardant

Material Notes: Characteristic: Good heat stability, good toughness, no migrating, easy to process, high gloss

Applications: Flame-retarded PS product

Appearance: Nature color particle

Information Provided by SPS (Guang Zhou) Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Thermal PropertiesMetricEnglishComments
Flammability, UL94 V-0V-0
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %
 
Descriptive Properties
7001RM4/PS Ratio1/4

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Meilian Chemical PE105B WHITE MASTERBATCH
LyondellBasell Aquathene® CM04482 Catalyst Masterbatch
KKPC Kumho KHS 65P High Styrene Resin Masterbatch (HSR)
Kazanorgsintez 107-30 KTU-2 Polyethylene Masterbatch, Carbon Black Filled
ICO Polymers ICOFLO™ 510-5018 400 Micron LDPE Powder

PSPS034 / 103389

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.