MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Schmelzer Industries Curveil 220-15 Fiberglass Veil
Categories: Ceramic; Glass; Glass Fiber; Other Engineering Material; Composite Fibers

Material Notes: Good for curved applications - drapable and flexible. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. The 200 series contains a binder additive. Data provided by the manufacturer, Schmelzer Industries.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Barcol 3434
Tensile Strength, Ultimate 20.91 MPa3033 psis.d. 2.20 MPa, test specimen 1.21 cm wide (s.d. 0.003 cm), 0.23 cm thick (s.d. 0.008 cm)
Elongation at Break 0.57 %0.57 %Elongation at max. load, 0.56%
Elongation at Yield 0.56 %0.56 %
Modulus of Elasticity 4.43 GPa643 ksistd. dev. 0.33 GPa
Flexural Strength 37.03 MPa5371 psis.d. 2.32 MPa, specimen 2.51 cm wide (s.d. 0.02 cm), 0.24 cm thick (s.d.008 cm), 3.8 cm span (s.d. 0 cm). Test conditions: Humidity 50%, Temp. 23°C.
Flexural Modulus 3.10 GPa450 ksiTangent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
E-Glass Fiber, Generic
Isoflon Tisoflon® 3 AD Polytetrafluoroethylene Coated Glass Fabric
Isoflon Tisoflon® 6 AD EXTRA SMOOTH Polytetrafluoroethylene Coated Glass Fabric
Schmelzer Industries Pearlveil 110-30 Fiberglass Veil
Envalior TEPEX® dynalite 408-C200(2)-FG290(2)/45% Carbon – Filament Glass – TPU Consolidated Composite Laminate

SI0001 / 74486

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.