MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dover Chemical PRIME BURNING LARD OIL Lard Oil, Lubricity Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Prime Burning Lard Oil (PBLO) is a lubricity additive ideal for use in conventional cutting oils and soluble oils for all types of machining operations. This additive enhances a fluid’s wetting characteristics and boundary lubricity, which causes reduced friction at the tool/work piece interface and improved surface finish. PBLO’s low level of free fatty acid makes it resistant to oxidation. This reduces the amount of oxidative degradation that can be caused by higher temperature machining operations.

Information provided by DoverChem

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.915 g/cc
@Temperature 15.6 °C
0.915 g/cc
@Temperature 60.0 °F
60/60°F
Saybolt Viscosity at 100°F 195 SUS195 SUS
Kinematic Viscosity at 40°C (104°F) 40 cSt40 cSt
ASTM Color 1.51.5
 
Chemical PropertiesMetricEnglishComments
Total Acid Number 1.01.0[mgKOH/g]
 
Thermal PropertiesMetricEnglishComments
Pour Point <= 7.22 °C<= 45.0 °F
Flash Point >= 315 °C>= 599 °FCOC

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dover Chemical MAYCO BASE 1210 Sulfurized Lard Oil, Non-Staining Sulfurized Additive
Dover Chemical EWS LARD OIL Lubricity Additive
Dover Chemical BASE 107 Sulfurized Lard Oil Active Sulfurized Additive
Dover Chemical BASE 101 Sulfurized Lard Oil, Lubricity/Extreme Pressure Additive

WDOVER130 / 217749

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.