MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CRP Technology AMC225xe Aluminum Alloy - SiC Composite, T4 Condition
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Aluminum Alloy; 2000 Series Aluminum Alloy

Material Notes: AMC225xe is a high quality aerospace grade aluminum alloy (AA2124) reinforced with 25% by volume of ultrafine particles of silicon carbide. It is manufactured by a special powder metallurgy route using a proprietary high-energy mixing process which ensures excellent particle distribution and enhances mechanical properties. The key benefits of AMC225xe for structural applications include: weight saving; increased component stiffness; and high fatigue resistance.

The combination of properties achieved with AMC225xe provides the potential for outstanding structural performance in a wide range of markets and applications including:

Motorsport

  • Performance valve train
  • Cylinder liners
  • Pistons
  • Connecting rods
  • Brake callipers
  • Disk Bells
  • Suspension parts
Aerospace & Defense
  • Aero engine vanes
  • Aircraft structure
  • Brakes and Wheels
  • Control Systems
  • Valve Blocks

Information provided by CRP Technology.

Vendors:   About CRP Technology
CRP Technology (Modena, Italy) develops, manufactures and sells its proprietary high performance composite materials Windform® for professional 3D Printing. It is also distinguished by its know-how in Selective Laser Sintering technology. It offers part production for short- and low-run production, and prototyping services with Windform®. Its specific application fields including but are not limited to: automotive and motorsports, design, aerospace, UAVs, marine, entertainment, defense, and packaging.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.88 g/cc0.104 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 210210HV10
Tensile Strength, Ultimate  65.0 MPa
@Temperature 350 °C
9430 psi
@Temperature 662 °F
short term exposure
 194 MPa
@Temperature 260 °C
28100 psi
@Temperature 500 °F
short term exposure
 530 MPa
@Temperature 200 °C
76900 psi
@Temperature 392 °F
short term exposure
 616 MPa
@Temperature 150 °C
89300 psi
@Temperature 302 °F
short term exposure
 650 MPa
@Temperature 20.0 °C
94300 psi
@Temperature 68.0 °F
Tensile Strength, Yield  48.0 MPa
@Temperature 350 °C
6960 psi
@Temperature 662 °F
short term exposure
 128 MPa
@Temperature 260 °C
18600 psi
@Temperature 500 °F
short term exposure
 448 MPa
@Temperature 200 °C
65000 psi
@Temperature 392 °F
short term exposure
 474 MPa
@Temperature 150 °C
68700 psi
@Temperature 302 °F
short term exposure
 480 MPa
@Temperature 20.0 °C
69600 psi
@Temperature 68.0 °F
Elongation at Break 5 %5 %
Modulus of Elasticity  84.0 GPa
@Temperature 300 °C
12200 ksi
@Temperature 572 °F
 92.0 GPa
@Temperature 250 °C
13300 ksi
@Temperature 482 °F
 102 GPa
@Temperature 200 °C
14800 ksi
@Temperature 392 °F
 108 GPa
@Temperature 150 °C
15700 ksi
@Temperature 302 °F
 115 GPa
@Temperature 20.0 °C
16700 ksi
@Temperature 68.0 °F
Poissons Ratio 0.300.30
Fatigue Strength  305 MPa
@# of Cycles 1.00e+7
44200 psi
@# of Cycles 1.00e+7
R=-1; Kt=1; Rotating Bend
 340 MPa
@# of Cycles 1.00e+6
49300 psi
@# of Cycles 1.00e+6
R=-1; Kt=1; Rotating Bend
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000082 ohm-cm0.0000082 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear  13.4 µm/m-°C
@Temperature -75.0 °C
7.44 µin/in-°F
@Temperature -103 °F
 14.8 µm/m-°C
@Temperature -25.0 °C
8.22 µin/in-°F
@Temperature -13.0 °F
 16.0 µm/m-°C
@Temperature 20.0 °C
8.89 µin/in-°F
@Temperature 68.0 °F
 17.6 µm/m-°C
@Temperature 75.0 °C
9.78 µin/in-°F
@Temperature 167 °F
Specific Heat Capacity 0.836 J/g-°C0.200 BTU/lb-°F
Thermal Conductivity 150 W/m-K1040 BTU-in/hr-ft²-°F
Melting Point >= 548 °C>= 1020 °FSolidus
Solidus 548 °C1020 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 505 °C941 °FSolution Heat Treatment

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Forged Plate
Materion AMC225XE T4 Aluminum/Silicon Carbide MMC Extruded Bar
Materion SupremEX® 217XG Aluminum - Silicon Carbide Metal Matrix Composite, T6 CWQ Billet
Materion SupremEX® 225XE Aluminum - Silicon Carbide Metal Matrix Composite, T6 CWQ Billet
Titanium Ti-6Al-4V (Grade 5), Annealed

NCRPT45 / 130421

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.