MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Kotec Carbotex KG-30MRA Polycarbonate, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 30% Glass Filled

Material Notes: Features: Glass fiber 30% reinforced, Mold release, Translucent, Dimensional stability, Flame retardant, High rigidity
Applications: OA equipment, Communications, Precision parts, Machineries, E & E parts

Information provided by Kotec Corporation

Key Words: PC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.43 g/cc1.43 g/ccASTM D792
Water Absorption 0.20 %
@Temperature 23.0 °C,
Time 86400 sec
0.20 %
@Temperature 73.4 °F,
Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 - 0.0040 cm/cm0.0020 - 0.0040 in/inASTM D995
Linear Mold Shrinkage, Transverse 0.0030 - 0.0050 cm/cm0.0030 - 0.0050 in/inASTM D995
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 127 MPa18400 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Strength 162 MPa23500 psiASTM D790
Flexural Modulus 7.55 GPa1100 ksiASTM D790
Izod Impact, Notched 1.00 J/cm
@Temperature 23.0 °C
1.87 ft-lb/in
@Temperature 73.4 °F
V-Notched 1/8"; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant 3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm508 kV/inASTM D149
Dissipation Factor 0.00080
@Frequency 1e+6 Hz
0.00080
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 110 sec110 secASTM D495
 
Thermal PropertiesMetricEnglishComments
Heat Distortion Temperature 146 °C295 °FASTM D648
Flammability, UL94 V-0
@Thickness 3.00 mm
V-0
@Thickness 0.118 in
 
Descriptive Properties
Light TransmittanceTranslucent3.0mm, ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI Latilon 28D G/30 PC, 30% Glass Fiber Reinforced
Cheng Yu Plastic ML3430 PC, 30% Glass Fiber
A. Schulman Matrixx 50S5302 Polycarbonate, 30% Glass Reinforced
LG Chemical LUPOY SC2302 PC+GF30%, High Impact
Overview of materials for Nylon 46, Unreinforced

PKOTEC034 / 93264

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.