MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Hostaform® C 13031 XF POM, Specialty
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Hostaform« acetal copolymer grade C13031 XF is an acetal copolymer modified to resist deterioration from aggressive fuel blends. This material is specially targeted for transportation industry fuel systems. In natural form, Hostaform« C13031 XF has a distinctive yellow color (Color code 50/5339) to denote use for fuel systems. Additionally the product is available in black 10/9022 for laser welding applications.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.42 g/cc0.0513 lb/in³ISO 1183
Linear Mold Shrinkage, Flow 0.022 cm/cm0.022 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.019 cm/cm0.019 in/inISO 294-4
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 190 °C
12 g/10 min
@Load 4.76 lb,
Temperature 374 °F
[cm3/10min]; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 62.0 MPa8990 psi50mm/min; ISO 527-2/1A
Elongation at Break 30 %30 %
Elongation at Yield 11 %11 %50mm/min; ISO 527-2/1A
Tensile Modulus 2.85 GPa413 ksi50mm/min; ISO 527-2/1A
Flexural Modulus 2.90 GPa421 ksiISO 178
Charpy Impact Unnotched 15.0 J/cm²71.4 ft-lb/in²ISO 179/1eU
 14.0 J/cm²
@Temperature -30.0 °C
66.6 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.750 J/cm²3.57 ft-lb/in²ISO 179/1eA
 0.600 J/cm²
@Temperature -30.0 °C
2.86 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C50.0 µin/in-°FISO 11359-2
Melting Point 170 °C338 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 159 °C318 °FISO 75-1, -2
Deflection Temperature at 1.8 MPa (264 psi) 102 °C216 °FISO 75-1, -2
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 120 °C176 - 248 °Fcavity
 190 - 210 °C374 - 410 °Fhot runner
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Zone 1 170 - 180 °C338 - 356 °F
Zone 2 180 - 190 °C356 - 374 °F
Zone 3 190 - 200 °C374 - 392 °F
Zone 4 190 - 210 °C374 - 410 °F
Die Temperature 190 - 210 °C374 - 410 °F
Melt Temperature 190 - 210 °C374 - 410 °F
Drying Temperature 80.0 - 100 °C176 - 212 °F
Dry Time 3.00 hour3.00 hour
Injection Pressure 60.0 - 120 MPa8700 - 17400 psi
Hold Pressure 60.0 - 120 MPa8700 - 17400 psi
Back Pressure <= 4.00 MPa<= 580 psi
Screw Speed  70 rpm
@Diameter 55.0 mm
70 rpm
@Diameter 2.17 in
 100 rpm
@Diameter 40.0 mm
100 rpm
@Diameter 1.57 in
 150 rpm
@Diameter 25.0 mm
150 rpm
@Diameter 0.984 in
 
Descriptive Properties
Injection moldingYes
Injection speedslow-medium
Processing conditions acc. ISO9988-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hostaform® C 13031 POM, Unfilled
Celanese Hostaform® EC270TX POM, Specialty
Celanese Hostaform® C 13031 XF 50/5339 Acetal Copolymer
BASF Ultraform® S 1320 0021 UNC POM
Celanese Hostaform® C 9021 POM, Unfilled

PHCQ321 / 178776

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.