MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

A. Schulman POLYAXIS® LPA815 LPA 815EVA
Categories: Polymer; Thermoplastic; Ethylene Vinyl Acetate; Ethylene Vinyl Acetate; Molded/Extruded

Material Notes: Description

Polyaxis LPA 815 is an EVA which is soft an pliable, even at low temperatures.

NOTE: Physical properties are based on rotationally molded samples from unpigmented resin. Density and ESCR tests were performed on compression molded samples.
Application

Applications of Polyaxis® LPA 815 include toys, dock bumpers and floats.
Information provided by A. Schulman.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.935 g/cc0.935 g/ccASTM D792
Vinyl Acetate Content 15 %15 %by weight
Melt Index of Compound 6.0 - 8.0 g/10 min6.0 - 8.0 g/10 min2.16/190; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 14.5 MPa2100 psi2"/min; ASTM D638
Elongation at Break 700 %700 %2"/min; ASTM D638
Flexural Modulus, 1% Secant 59.3 MPa8600 psiASTM D790

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Ateva® 1241 EVA polymer for compounds, flexible packaging and foam
Celanese Ateva® 1807EG Medical Grade EVA
Celanese Ateva® 2606A EVA polymer for adhesives, automotive, compounds and molding
A. Schulman Alcryn® 2265 UT Melt Processable Rubber
Arkema Orevac® 18216 Maleic Anhydride modified EVA

PASHU064 / 25028

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.