MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Techmer ES Electrafil® J-1/CF/20 Nylon 66, 20% Carbon Fiber Reinforced
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 20% Carbon Fiber Filled

Material Notes:

Key Words: Polyamide 66
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.23 g/cc0.0444 lb/in³ASTM D792
Water Absorption 1.0 %1.0 %24 hrs. ASTM D570
Linear Mold Shrinkage 0.0020 cm/cm
@Thickness 3.17 mm
0.0020 in/in
@Thickness 0.125 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell E 6767ASTM D785
Tensile Strength, Ultimate 193 MPa28000 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Tensile Modulus 13.8 GPa2000 ksiASTM D638
Flexural Yield Strength 290 MPa42000 psiASTM D790
Flexural Modulus 15.2 GPa2200 ksiASTM D790
Compressive Strength 172 MPa25000 psiASTM D695
Shear Strength 82.7 MPa12000 psiASTM D732
Izod Impact, Notched 0.694 J/cm
@Thickness 3.17 mm
1.30 ft-lb/in
@Thickness 0.125 in
ASTM D256
Izod Impact, Unnotched 5.34 J/cm
@Thickness 3.17 mm
10.0 ft-lb/in
@Thickness 0.125 in
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 10.0 - 100 ohm-cm10.0 - 100 ohm-cmASTM C611
Surface Resistance 1000 - 10000 ohm1000 - 10000 ohmASTM D4496
 
Thermal PropertiesMetricEnglishComments
CTE, linear 18.0 µm/m-°C
@Temperature 20.0 °C
10.0 µin/in-°F
@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 260 °C500 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 254 °C490 °FASTM D648
Flammability, UL94 HB
@Thickness 1.59 mm
HB
@Thickness 0.0625 in

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Cast Nylons Nycast® GF 30% Glass Filled Cast Nylon
RTP Company RTP 105 FR  Polypropylene (PP) Glass Fiber 30% - Flame Retardant
Ensinger HYDLAR® Z Nylon, Pultruded Aramid Fiber Reinforced (PA)
Solvay CYCOM® 919 Epoxy Prepreg with Kevlar 49 Aramid Fiber, Weave Style 120
Solvay CYCOM® 5216 Epoxy - Woven Aramid Fiber Prepreg

PTLCOM008 / 70572

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.