MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol ESTANE® 58315 Ether Based Thermoplastic Polyurethane
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP; Thermoplastic Polyurethane, Elastomer, Ether Grade

Material Notes: Features: Very good physical properties, hydrolysis resistance, low temperature performance and abrasion. Wide processing window for extrusion.

Uses: Blown and flat die/cast film extrusion, Injection molding and cable jacketing.

Available in Americas, Europe, Middle East, Africa, India and Asia

Information provided by Lubrizol.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.12 g/cc1.12 g/ccASTM D792
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 82 - 88
@Time 5.00 sec
82 - 88
@Time 0.00139 hour
ASTM D2240
Tensile Strength 48.3 MPa7010 psiASTM D412
 33.81 MPa
@Temperature 75.0 °C,
Time 4.838e+6 sec
4904 psi
@Temperature 167 °F,
Time 1344 hour
30 Mil Sheet, Immersion in Water
 39.12 MPa
@Temperature 75.0 °C,
Time 605000 sec
5674 psi
@Temperature 167 °F,
Time 168 hour
30 Mil Sheet, Immersion in Water
 39.12 MPa
@Temperature 75.0 °C,
Time 1.21e+6 sec
5674 psi
@Temperature 167 °F,
Time 336 hour
30 Mil Sheet, Immersion in Water
 46.85 MPa
@Temperature 75.0 °C,
Time 2.82e+6 sec
6795 psi
@Temperature 167 °F,
Time 784 hour
30 Mil Sheet, Immersion in Water
 48.3 MPa
@Temperature 75.0 °C,
Time 0.000 sec
7010 psi
@Temperature 167 °F,
Time 0.000 hour
30 Mil Sheet, Immersion in Water
Elongation at Break 570 %570 %ASTM D412
100% Modulus 6.20 MPa
@Strain 100 %
899 psi
@Strain 100 %
ASTM D412
300% Modulus 10.3 MPa
@Strain 300 %
1490 psi
@Strain 300 %
ASTM D412
Tear Strength 26.3 kN/m150 pliTrosuer; ASTM D470
Graves Tear Strength 85.9 kN/m490 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 3737H18, 1000g; ASTM D3389 B
Tensile Set 14 %14 %200% elongation; ASTM D412
 
Thermal PropertiesMetricEnglishComments
Melting Point 135 °C275 °FDSC
 145 °C293 °FKofler
Glass Transition Temp, Tg -50.0 °C-58.0 °FDSC
 
Optical PropertiesMetricEnglishComments
Haze 1.8 %1.8 %pressed between glass; ASTM D1003
 
Processing PropertiesMetricEnglishComments
Zone 1 171 °C340 °FExtrusion
Zone 2 177 °C351 °FExtrusion
Zone 3 182 °C360 °FExtrusion
Zone 4 188 °C370 °FExtrusion
Adapter Temperature 188 °C370 °F5, Extrusion
Die Temperature 188 °C370 °F6, Zone 1, Extrusion
 188 °C370 °FZone 2, Extrusion
Drying Temperature 104 °C219 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol ESTANE® 58887 Ether Based Thermoplastic Polyurethane
Covestro Bayblend® FR 3000 HI Polycarbonate + ABS, Flame Retardant Grade
Lubrizol ESTANE® 58137 Ester Based Thermoplastic Polyurethane
Lubrizol Advanced Materials PEARLTHANE® Clear 15N85 Thermoplastic Polyurethane Elastomer
LG Chemical TR557 MABS, High Transparency, High Impact

PNOVEON049 / 55316

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.