MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay Vac-Pak® E3760 PVF Release Film
Categories: Polymer; Film; Thermoplastic; Fluoropolymer

Material Notes: Description: Release film. Ideally suited to mild contour and flat panel applications.

Features & Benefits:

  • Excellent for mild contour and flat parts as it will lie flat and smooth, with little wrinkling issues, as experience with other, more pliable, release films
  • Available perforated or non-perforated

Information provided by Cytec, subsequently acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 25.0 microns0.984 mil
 50.0 microns1.97 mil
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 68.9 MPa10000 psi
Elongation at Break 200 %200 %
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C399 °F
 
Descriptive Properties
ColorClear and white
Yield28.6 m2/kg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont™ Tedlar® SP TTR5JAM9 Transparent Polyvinyl Fluoride Film
Goodfellow Polyvinyl Fluoride (PVF) Film
DuPont Elvanol® T-25 Polyvinyl Alcohol Textile Grade
DuPont™ Tedlar® SP TUA10AH9 Polyvinyl Fluoride Film
Eastman Saflex® PA11 PVB Encapsulant High Flow Formulations

PCYTED277 / 180579

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.