MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TechnylStar™ SX 218 V50 BK 38N-K PA6, 50% glass filled, CONDITIONED
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: Description: High stiffness materials Technylstar polyamide 6, reinforced with 50% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.

Available in: Asia Pacific

Product Applications: Due to its outstanding flow characteristics, TECHNYLSTAR SX 218 V50 BLACK 38N-K provides a significant productivity improvement and allows more freedom in mold design and part design versus a standard polyamide solution. This grade is used in automotive and industrial parts, demanding high mechanical strength, good UV resistance and excellent surface aspect. This product is suitable for side mirror base plate, brackets and housings for electrical parts. This product is available in black color.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.55 g/cc0.0560 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 162 MPa23500 psi ISO 527 Type 1A
Elongation at Break 4.0 %4.0 %ISO 527 Type 1A
Tensile Modulus 11.6 GPa1680 ksiISO 527 Type 1A
Flexural Modulus 10.0 GPa1450 ksiASTM D790
Izod Impact, Notched (ISO) 22.0 kJ/m²10.5 ft-lb/in²ISO 180/1U
Izod Impact, Unnotched (ISO) 100 kJ/m²47.6 ft-lb/in²ISO 180/1U
Charpy Impact Unnotched 9.50 J/cm²45.2 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 2.00 J/cm²9.52 ft-lb/in²ISO 179/1eA
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone235-240°C
Mixing Zone240-245°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TechnylStar™ SX 218 V50 BK 38N-K PA6, 50% glass filled, DRY
Domo TechnylStar™ SX 218 V50 PA6, 50% glass filled, Conditioned
Domo TechnylStar™ SX 218 V50 PA6, 50% glass filled
Envalior Durethan® BKV 60 H2.0 EF DUS060 900116 Nylon 6 (PA6), 60% Glass Fiber Reinforced, Conditioned
Domo Technyl® C 218 V50 50% Glass Filled, Heat Stabilized Nylon 6

PRHOD84a / 186442

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.