MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

SK Chemicals Saran® 506 Polymer  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyvinyl Dichloride (PVDC)

Material Notes: Saran™ 506 Polymer is designed as an ignition resistant adhesive bonding agent. Saran™ 506 is a vinylidene chloride copolymer supplied as a white, micronized powder. It is unaffected by humidity, and has outstanding adhesion to fibrous substrates.

No expressed data on flammability are to be considered indications of behavior of this material in actual fire situations; virtually all organic materials burn when sufficient heat and oxygen are supplied.

SK Global Chemical has purchased the SARAN® resin business from Dow.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.400 - 0.561 g/cc0.0145 - 0.0203 lb/in³Dow Method
Particle Size 15 - 25 µm15 - 25 µmDow Method
 
Thermal PropertiesMetricEnglishComments
Melting Point 114 - 172 °C237 - 342 °FDow Method (DSC)
Oxygen Index 63 - 77 %63 - 77 %ASTM D2863
 
Optical PropertiesMetricEnglishComments
Optical Density 0.26 - 2.60.26 - 2.6[Dm]; Flaming Mode; NBS Chamber
 0.33 - 2.930.33 - 2.93[Dm]; Smoldering Mode; NBS Chamber

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyvinyl Dichloride (PVDC)
SK Chemicals Saran® 168
SK Chemicals Saran® 2032
SK Chemicals Saran® 313 PVDC
SK Chemicals Saran® 540 Clear Plastic Barrier Film

PDOW1413 / 30631

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.