MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Borealis FR4845 Irradiation Crosslinkable Polyethylene Compound
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: FR4845 is an Irradiation Crosslinkable non-halogen flame retardant compound developed for the automotive wire market. Applications: FR4845 is intended for use as a 125º C rated primary insulation for crosslinked automotive wire. Specifications: FR4845 in combination meets these applicable requirements when processed using sound extrusion and testing procedure: SAE J1128/J1127

Information provided by Borealis AG

Key Words: PE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.40 g/cc0.0506 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 13.8 MPa2000 psiASTM D412
Elongation at Break 180 %180 %ASTM D412
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+6 ohm-cm1.00e+6 ohm-cmASTM D257
Dielectric Constant 3.7
@Frequency 6e+7 Hz
3.7
@Frequency 6e+7 Hz
ASTM D150
Dielectric Strength >= 21.7 kV/mm>= 551 kV/inASTM D149
Dissipation Factor 0.010
@Frequency 6e+7 Hz
0.010
@Frequency 6e+7 Hz
ASTM D150
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature <= -40.0 °C<= -40.0 °FASTM D2863
 
Processing PropertiesMetricEnglishComments
Middle Barrel Temperature 127 °C261 °Fbarrel 1
 149 °C300 °Fbarrel 6
Melt Temperature 160 - 165 °C320 - 329 °F
Drying Temperature 60.0 °C140 °Fhumidified air drying temperature;2-8h
Shelf Life 12.0 Month12.0 Month
 
Descriptive Properties
Single Vertical Flame TestPass20AWG;ISO 6722/SAE J1128

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
A-Glass Fiber, Generic
Borealis Visico™ LE4423/LE4460/LE4437 Scorch Retardant, Moisture-Crosslinking Polyethylene Compound for Low Voltage Installation
Borealis HE1878E High Density Polyethylene Powder for Crosslinked Pipes
Borealis FR4837 Chemically Crosslinkable Polyethylene Compound for Primary Automotive Wires
Crystex Composites Mykroy/Mycalex MM 400 Machining Grade Glass-bonded Mica Composite

PBOREA448 / 108707

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.