MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sichuan Deyang Haton® hGR20 Polyphenylene Sulfide, Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 20% Glass Fiber Filler

Material Notes: Injection molding

Information provided by Sichuan Deyang Chemical Co., LTD

Key Words: UL E236625
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.30 g/cc0.0470 lb/in³GB/T 1033.1-2008
Water Absorption 0.020 %0.020 %GB/T 1034-2008
Linear Mold Shrinkage, Flow 0.0025 cm/cm0.0025 in/inGB/T 15585-1995
Linear Mold Shrinkage, Transverse 0.0075 cm/cm0.0075 in/inGB/T 15585-1995
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell L 102102GB/T 3398.2-2008
Tensile Strength 130 MPa18900 psiGB/T 1040.2-2006
Elongation at Break 1.8 %1.8 %GB/T1040.2-2006
Flexural Strength 190 MPa27600 psiGB/T 9341-2008
Flexural Modulus 9.10 GPa1320 ksiGB/T 9341-2008
Izod Impact, Notched (ISO) 9.60 kJ/m²4.57 ft-lb/in²GB/T 1843-2008
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.20e+16 ohm-cm2.20e+16 ohm-cmGB/T1410-2006
Surface Resistivity per Square 9.80e+15 ohm9.80e+15 ohmGB/T1410-2006
Dielectric Constant 3.23.2GB/T 1409-2006
Dielectric Strength 16.0 kV/mm406 kV/inGB/T1408.1-2006
Dissipation Factor 0.00200.0020GB/T 1409-2006
 
Thermal PropertiesMetricEnglishComments
Melting Point 280 °C536 °FGBT/T 19466.3-2004
Deflection Temperature at 1.8 MPa (264 psi) 265 °C509 °FGB/T 1634.2-2004
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese FORTRON 1140L0 PPS, 40% Glass Reinforced
Sichuan Deyang Haton® hGR60 Polyphenylene Sulfide, Glass Fiber Reinforced
Sichuan Deyang Haton® hGR40 Polyphenylene Sulfide, Glass Fiber Reinforced
Celanese Fortron® 1140 L4 Polyphenylene Sulfide (PPS), 40% Glass Fiber

PSICHU901 / 156142

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.