MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Aleris Hokotol Aluminum Alloy, 325 mm Thickness
Categories: Metal; Nonferrous Metal; Aluminum Alloy; 7000 Series Aluminum Alloy

Material Notes: Sample treatment not specified for property data.

Applications include molds for blow forming and injection molding for plastics; bolsters and force plates; high strength/low weight machine parts; and mechanical components with elevated mechanical properties. Poor weldability and corrosion resistance. Very good machinability.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.83 g/cc0.102 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 180180
Hardness, Knoop 232232Estimated from Brinell
Hardness, Rockwell A 5959Estimated from Brinell
Hardness, Rockwell B 9696Estimated from Brinell
Hardness, Vickers 217217Estimated from Brinell
Tensile Strength, Ultimate >= 450 MPa>= 65300 psiMinimum
 485 MPa70300 psiTypical
Tensile Strength, Yield  >= 390 MPa
@Strain 0.2 %
>= 56600 psi
@Strain 0.2 %
Minimum
 415 MPa
@Strain 0.2 %
60200 psi
@Strain 0.2 %
Typical
Elongation at Break >= 1.0 %>= 1.0 %Minimum
 2.0 %2.0 %Typical
Modulus of Elasticity 70.3 GPa10200 ksi
Machinability 90 %90 %
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000430 ohm-cm0.00000430 ohm-cm
 
Thermal PropertiesMetricEnglishComments
CTE, linear 23.5 µm/m-°C
@Temperature 20.0 - 100 °C
13.1 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 154 W/m-K1070 BTU-in/hr-ft²-°F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 86 - 90.9 %86 - 90.9 %as balance
Chromium, Cr <= 0.10 %<= 0.10 %
Copper, Cu 1.5 - 2.6 %1.5 - 2.6 %
Iron, Fe <= 0.30 %<= 0.30 %
Magnesium, Mg 1.8 - 2.6 %1.8 - 2.6 %
Manganese, Mn <= 0.15 %<= 0.15 %
Other, total <= 0.15 %<= 0.15 %
Silicon, Si <= 0.20 %<= 0.20 %
Titanium, Ti <= 0.060 %<= 0.060 %
Zinc, Zn 5.7 - 7.6 %5.7 - 7.6 %
Zirconium, Zr 0.080 - 0.25 %0.080 - 0.25 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aleris Hokotol Aluminum Alloy, 100 mm Thickness
Aleris Hokotol Aluminum Alloy, 300 mm Thickness
Aleris Hokotol Aluminum Alloy, 200 mm Thickness
ALIMEX ACP 6000 Aluminum Cast Plate
PCP-Canada ALCA 5® 5083 Cast Aluminum Mold Plate

NHOOG13 / 159724

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.