MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Latrobe Lescalloy® AF 1410 VIM-VAR ; 6 in High Strength Alloy Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel

Material Notes: LESCALLOY AF1410 VIM-VAR steel exhibits both high strength and very high fracture toughness. It is typically used in the 235/260 ksi (1620/1793 MPa) tensile strength range for a variety of critical, fracture-sensitive aerospace structural applications. It is double vacuum melted (VIM-VAR…vacuum induction melted followed by vacuum arc remelting) to provide superior cleanliness, ingot homogeneity, and to enhance mechanical properties.

Heat Treatment - 857°C - 1 hour oil quench; -73°C - 1 hr air warm; 510°C - 5 hrs air cool

Information Provided by Timken Latrobe Steel.

Timken sold Latrobe in December 2006. They are now Latrobe Specialty Steels Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.83 g/cc0.283 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1670 MPa242000 psiTransverse
 1670 MPa242000 psiLongitudinal
Tensile Strength, Yield 1517 MPa220000 psiTransverse
 1517 MPa220000 psiLongitudinal
Elongation at Break 17 %17 %Longitudinal
 17 %17 %Transverse
Reduction of Area 70 %70 %Transverse
 73 %73 %Longitudinal
Modulus of Elasticity 203 GPa29400 ksi
Fracture Toughness 165 MPa-m½150 ksi-in½
Charpy Impact 76.0 J56.1 ft-lbV-Notch, Transverse
 84.0 J62.0 ft-lbV-Notch, Longitudinal
 
Processing PropertiesMetricEnglishComments
Processing Temperature 168 °C334 °FMartensitic Finish
 336 °C637 °FMartensitic Start
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.15 %0.15 %
Chromium, Cr 2.0 %2.0 %
Cobalt, Co 14 %14 %
Iron, Fe 72.65 %72.65 %
Manganese, Mn 0.10 %0.10 %
Molybdenum, Mo 1.0 %1.0 %
Nickel, Ni 10 %10 %
Silicon, Si 0.10 %0.10 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Latrobe Lescalloy® 300M - HS VAC-ARC High Strength Alloy Steel
Latrobe Lescalloy® HP 9-4-30 VAC-ARC ; 13.5 in RCS Billet Size High Strength Alloy Steel
QuesTek® Innovations Ferrium® C61™ Case-hardened Gear Steel with Ultrahigh-strength Core
AISI Grade 18Ni (300) Maraging Steel, Aged, round bar, tested longitudinal, 16 mm
Latrobe Lescalloy® HY-TUF VAC-ARC High Strength Alloy Steel

NTIMK028 / 19376

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.