Physical Properties | Metric | English | Comments |
---|
Density | 1.32 g/cc @Temperature 23.0 °C | 0.0477 lb/in³ @Temperature 73.4 °F |
Filler Content | 30 % | 30 % |
Moisture Absorption | 2.0 - 2.2 % @Temperature 70.0 °C | 2.0 - 2.2 % @Temperature 158 °F |
Water Absorption at Saturation | 5.7 - 6.3 % @Time 82800 sec | 5.7 - 6.3 % @Time 23.0 hour |
Linear Mold Shrinkage, Flow | 0.0024 cm/cm | 0.0024 in/in |
Linear Mold Shrinkage, Transverse | 0.013 cm/cm | 0.013 in/in |
Spiral Flow | 89.0 cm | 35.0 in |
|
Mechanical Properties | Metric | English | Comments |
---|
Ball Indentation Hardness | 225 MPa | 32600 psi |
Tensile Strength at Break | 185 MPa | 26800 psi |
| 92.5 MPa @Treatment Temp. 160 - 175 °C, Time 1.80e+7 sec | 13400 psi @Treatment Temp. 320 - 347 °F, Time 5000 hour |
| 92.5 MPa @Treatment Temp. 130 - 150 °C, Time 7.20e+7 sec | 13400 psi @Treatment Temp. 266 - 302 °F, Time 20000 hour |
Elongation at Break | 3.6 % | 3.6 % |
Tensile Modulus | 8.50 GPa | 1230 ksi |
Flexural Strength | 260 MPa | 37700 psi |
Flexural Modulus | 7.60 GPa | 1100 ksi |
Charpy Impact Unnotched | 6.40 J/cm² @Temperature -30.0 °C | 30.5 ft-lb/in² @Temperature -22.0 °F |
| 7.00 J/cm² @Temperature 23.0 °C | 33.3 ft-lb/in² @Temperature 73.4 °F |
Charpy Impact, Notched | 0.900 J/cm² @Temperature -30.0 °C | 4.28 ft-lb/in² @Temperature -22.0 °F |
| 1.00 J/cm² @Temperature 23.0 °C | 4.76 ft-lb/in² @Temperature 73.4 °F |
|
Electrical Properties | Metric | English | Comments |
---|
Volume Resistivity | 1.00e+13 ohm-cm | 1.00e+13 ohm-cm |
Surface Resistance | 1.00e+12 ohm | 1.00e+12 ohm |
Comparative Tracking Index | 600 V | 600 V |
|
Thermal Properties | Metric | English | Comments |
---|
Melting Point | 262 °C | 504 °F |
Deflection Temperature at 0.46 MPa (66 psi) | 260 °C | 500 °F |
Deflection Temperature at 1.8 MPa (264 psi) | 255 °C | 491 °F |
Flammability, UL94 | HB @Thickness 1.60 mm | HB @Thickness 0.0630 in |
Glow Wire Flammability Index | 650 °C @Thickness 1.60 mm | 1200 °F @Thickness 0.0630 in |
|
Processing Properties | Metric | English | Comments |
---|
Feed Temperature | 60.0 - 80.0 °C | 140 - 176 °F |
Nozzle Temperature | 280 - 295 °C | 536 - 563 °F |
Zone 1 | 260 - 300 °C | 500 - 572 °F |
Zone 2 | 260 - 300 °C | 500 - 572 °F |
Zone 3 | 260 - 300 °C | 500 - 572 °F |
Zone 4 | 260 - 300 °C | 500 - 572 °F |
Melt Temperature | 280 - 320 °C | 536 - 608 °F |
Mold Temperature | 80.0 - 100 °C | 176 - 212 °F |
Drying Temperature | 80.0 °C | 176 °F |
Dry Time | 2.00 hour | 2.00 hour |
Hold Pressure | 30.0 - 80.0 MPa | 4350 - 11600 psi |
Back Pressure | 5.00 - 10.0 MPa | 725 - 1450 psi |
|
Descriptive Properties |
---|
Rate acc. FMVSS 302 (<100/min) | Passed |
Rate acc. FMVSS 302,(<100/min) | FMVSS 302, >1 [mm] Thickness |
Resistance to Oleic acid | Pass |
Resistance to Acetaldehyde | Fail |
Resistance to Acetic Acid | Pass |
Resistance to Acetone | Pass |
Resistance to Acetonitrile | Pass |
Resistance to Acrylonitrile | Pass |
Resistance to Allyl alcohol | Fail |
Resistance to Amyl alcohol | Pass |
Resistance to Aqueous Ammonia | Pass |
Resistance to Benzene | Fail |
| Pass |
| Pass |
Resistance to Biodiesel | Pass |
Resistance to Boric acid | Fail |
| Pass |
Resistance to Brake fluid (DOT 4) | Fail |
| Pass |
Resistance to Calcium chloride, alcoholic | Fail |
Resistance to Calcium chloride, aqueous | Pass |
Resistance to Carbonic acid | Pass |
Resistance to Caustic potash solution, aqueous | Pass |
Resistance to Chlorine | Fail |
Resistance to Chlorine water | Fail |
Resistance to Chloroacetic acid | Fail |
Resistance to Chromic acid | Fail |
Resistance to Cyclohexane | Pass |
Resistance to Cyclohexanol | Pass |
Resistance to Dichloro-Acetic acid | Fail |
Resistance to Diesel fuel (DIN 51601) | Pass |
Resistance to Ethanol | Pass |
Resistance to Ethylene glycol/water | Fail |
Resistance to Formaldehyde, aqueous | Pass |
Resistance to Formic acid | Fail |
Resistance to Glycerin | Pass |
Resistance to Hydraulic oil H and HL (DIN 51524) | Pass |
Resistance to Hydrogen chloride, gas | Fail |
Resistance to Iso-octanol | Pass |
Resistance to Isopropanol | Pass |
Resistance to Methanol | Pass |
Resistance to Methylene chloride | Fail |
Resistance to Motor oil (SAE 10W-40) | Pass |
| Pass |
Resistance to Natural Gas | Pass |
Resistance to Nitric acid | Fail |
Resistance to Ozone | Fail |
Resistance to Phenol | Fail |
Resistance to Phosphoric acid | Fail |
Resistance to Potassium chloride, aqueous | Pass |
Resistance to Potassium permanganate, aqueous | Fail |
Resistance to Sodium chloride, aqueous | Pass |
Resistance to Sodium hydroxide solution, aqueous | Pass |
Resistance to Sodium hypochlorite, aqueous | Fail |
Resistance to Transmission oil (ATF m 1375.4) | Pass |
Resistance to Urea, aqueous | Pass |
Resistant to Carbon disulfide | Pass |
Resistant to Carbon tetrachloride | Pass |
Resistant to Citric acid | Pass |
Resistant to Ethyl acetate | Pass |
Resistant to Hydrochloric acid | Fail |
Resistant to Hydrogen peroxide | Fail |
Resistant to Seawater | Pass |
Resistant to Silicone fluid | Pass |
Resistant to Sodium hypochlorite, aqueous | Fail |
Resistant to Sulfuric acid | Fail |
| Fail |
Resistant to Super-grade petrol (DIN 51600) | Pass |
Resistant to Toluol | Pass |
Resistant to Water | Pass |
Resistant to Xylol | Pass |
Resistant to Zinc chloride, aqueous | Fail |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view