MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Elastomer, Melt-Processible Rubber

Material Notes: This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 0.100 - 1.99 g/cc0.00361 - 0.0717 lb/in³Average value: 1.02 g/cc Grade Count:757
 0.785 - 0.785 g/cc
@Temperature >=125 °C
0.0284 - 0.0284 lb/in³
@Temperature >=257 °F
Average value: 0.785 g/cc Grade Count:1
Water Absorption 0.300 - 0.700 %0.300 - 0.700 %Average value: 0.488 % Grade Count:8
Moisture Absorption at Equilibrium 3.30 - 3.30 %
@Temperature 80.0 - 80.0 °C
3.30 - 3.30 %
@Temperature 176 - 176 °F
Average value: 3.30 % Grade Count:1
Oxygen Transmission 53.0 - 64.0 cc-mm/m²-24hr-atm135 - 163 cc-mil/100 in²-24hr-atmAverage value: 58.0 cc-mm/m²-24hr-atm Grade Count:6
Viscosity 200 - 720000 cP200 - 720000 cPAverage value: 105000 cP Grade Count:7
 17.0 - 5800 cP
@Temperature 30.0 - 200 °C
17.0 - 5800 cP
@Temperature 86.0 - 392 °F
Average value: 1.49e+6 cP Grade Count:22
 4000 - 5.00e+7 cP
@Temperature 190 - 210 °C
4000 - 5.00e+7 cP
@Temperature 374 - 410 °F
Average value: 1.49e+6 cP Grade Count:117
 4000 - 5.00e+7 cP
@Shear Rate 0.100 - 11000 1/s
4000 - 5.00e+7 cP
@Shear Rate 0.100 - 11000 1/s
Average value: 1.49e+6 cP Grade Count:117
Mooney Viscosity 5.80 - 48.05.80 - 48.0Average value: 21.0 Grade Count:20
Linear Mold Shrinkage 0.000400 - 0.0420 cm/cm0.000400 - 0.0420 in/inAverage value: 0.0152 cm/cm Grade Count:287
Linear Mold Shrinkage, Transverse 0.00300 - 0.0392 cm/cm0.00300 - 0.0392 in/inAverage value: 0.0133 cm/cm Grade Count:37
Melt Flow 0.0800 - 170 g/10 min0.0800 - 170 g/10 minAverage value: 13.5 g/10 min Grade Count:487
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 2.00 - 98.02.00 - 98.0Average value: 63.7 Grade Count:708
Hardness, Shore D 16.0 - 80.016.0 - 80.0Average value: 45.7 Grade Count:91
Hardness, Shore OO 30.0 - 58.030.0 - 58.0Average value: 46.0 Grade Count:5
Tensile Strength, Ultimate 0.255 - 51.0 MPa37.0 - 7400 psiAverage value: 9.38 MPa Grade Count:650
 2.96475 - 43.5749 MPa
@Temperature -40.0 - 85.0 °C
430.001 - 6320.01 psi
@Temperature -40.0 - 185 °F
Average value: 23.3 MPa Grade Count:1
Tensile Strength, Yield 0.689 - 47.0 MPa100 - 6820 psiAverage value: 9.04 MPa Grade Count:152
Film Elongation at Break, MD 740 - 1270 %740 - 1270 %Average value: 1060 % Grade Count:7
Film Elongation at Break, TD 820 - 1200 %820 - 1200 %Average value: 1070 % Grade Count:7
Elongation at Break 9.50 - 1660 %9.50 - 1660 %Average value: 565 % Grade Count:755
 780 - 1360 %
@Temperature -40.0 - 85.0 °C
780 - 1360 %
@Temperature -40.0 - 185 °F
Average value: 1070 % Grade Count:1
Elongation at Yield 16.0 - 100 %16.0 - 100 %Average value: 46.8 % Grade Count:8
 10.0 - 10.0 %
@Temperature -35.0 - -35.0 °C
10.0 - 10.0 %
@Temperature -31.0 - -31.0 °F
Average value: 10.0 % Grade Count:2
Modulus of Elasticity 0.000300 - 2.26 GPa0.0435 - 327 ksiAverage value: 0.204 GPa Grade Count:70
Flexural Yield Strength 2.40 - 294 MPa348 - 42700 psiAverage value: 48.2 MPa Grade Count:28
Flexural Modulus 0.00207 - 2.26 GPa0.300 - 327 ksiAverage value: 0.246 GPa Grade Count:133
 0.0379212 - 2.07946 GPa
@Temperature -40.0 - 85.0 °C
5.50009 - 301.605 ksi
@Temperature -40.0 - 185 °F
Average value: 0.660 GPa Grade Count:2
Compressive Yield Strength 0.0900 - 2.33 MPa13.1 - 338 psiAverage value: 0.661 MPa Grade Count:10
Compressive Modulus 0.00220 - 0.00760 GPa0.319 - 1.10 ksiAverage value: 0.00416 GPa Grade Count:10
Resilience 5.00 - 67.05.00 - 67.0Average value: 35.6 Grade Count:12
Rebound 12.0 - 60.0 %12.0 - 60.0 %Average value: 36.6 % Grade Count:17
Poissons Ratio 0.490 - 0.5200.490 - 0.520Average value: 0.500 Grade Count:15
Shear Modulus 0.00119 - 0.0115 GPa0.173 - 1.67 ksiAverage value: 0.00413 GPa Grade Count:22
Secant Modulus 0.00336 - 0.110 GPa0.487 - 16.0 ksiAverage value: 0.0249 GPa Grade Count:41
Izod Impact, Notched 0.267 J/cm - NB0.500 ft-lb/in - NBAverage value: 2.43 J/cm Grade Count:22
 0.300 J/cm - NB
@Temperature -40.0 - -20.0 °C
0.562 ft-lb/in - NB
@Temperature -40.0 - -4.00 °F
Average value: 2.20 J/cm Grade Count:21
Gardner Impact 18.1 - 28.2 J13.3 - 20.8 ft-lbAverage value: 23.0 J Grade Count:4
 12.5074 - 137.051 J
@Temperature -30.0 - -6.67 °C
9.22501 - 101.083 ft-lb
@Temperature -22.0 - 20.0 °F
Average value: 37.9 J Grade Count:17
Dart Drop, Total Energy 271.164 - 474.537 J
@Temperature -40.0 - -40.0 °C
200.000 - 350.000 ft-lb
@Temperature -40.0 - -40.0 °F
Average value: 373 J Grade Count:1
Tear Strength Test 17.5 - 57017.5 - 570Average value: 284 Grade Count:11
Tear Strength 1.60 - 275 kN/m9.13 - 1570 pliAverage value: 34.1 kN/m Grade Count:517
 10.4 - 13.0 kN/m
@Temperature 100 - 100 °C
59.3 - 74.2 pli
@Temperature 212 - 212 °F
Average value: 12.4 kN/m Grade Count:4
Peel Strength 0.470 - 1.35 kN/m2.68 - 7.72 pliAverage value: 0.886 kN/m Grade Count:4
Graves Tear Strength 16.0 - 62.2 kN/m91.3 - 355 pliAverage value: 33.8 kN/m Grade Count:51
 9.00 - 10.2 kN/m
@Temperature 100 - 100 °C
51.4 - 58.2 pli
@Temperature 212 - 212 °F
Average value: 9.58 kN/m Grade Count:6
Taber Abrasion, mg/1000 Cycles 0.00130 - 5810.00130 - 581Average value: 84.9 Grade Count:72
Compression Set 3.90 - 100 %3.90 - 100 %Average value: 36.7 % Grade Count:325
Tensile Set 3.80 - 185 %3.80 - 185 %Average value: 24.8 % Grade Count:102
Film Tensile Strength at Break, MD 23.5 - 38.2 MPa3410 - 5540 psiAverage value: 35.2 MPa Grade Count:7
Film Tensile Strength at Break, TD 24.5 - 38.2 MPa3550 - 5540 psiAverage value: 31.0 MPa Grade Count:7
Torsional Stiffness 1.38 - 127 MPa200 - 18500 psiAverage value: 14.2 MPa Grade Count:20
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 5.30e+15 - 9.10e+16 ohm-cm5.30e+15 - 9.10e+16 ohm-cmAverage value: 3.57e+16 ohm-cm Grade Count:5
 9.70e+15 - 9.60e+16 ohm-cm
@Temperature 50.0 - 50.0 °C
9.70e+15 - 9.60e+16 ohm-cm
@Temperature 122 - 122 °F
Average value: 4.69e+16 ohm-cm Grade Count:3
Dielectric Constant 2.10 - 2.802.10 - 2.80Average value: 2.37 Grade Count:15
Dielectric Strength 19.6 - 38.2 kV/mm498 - 970 kV/inAverage value: 26.0 kV/mm Grade Count:14
Dissipation Factor 0.000100 - 0.005000.000100 - 0.00500Average value: 0.00161 Grade Count:4
 
Thermal PropertiesMetricEnglishComments
CTE, linear 119 - 147 µm/m-°C66.1 - 81.7 µin/in-°FAverage value: 132 µm/m-°C Grade Count:5
CTE, linear, Transverse to Flow 117 - 132 µm/m-°C65.0 - 73.3 µin/in-°FAverage value: 125 µm/m-°C Grade Count:4
Thermal Conductivity 0.159 - 0.159 W/m-K
@Temperature 205 - 205 °C
1.10 - 1.10 BTU-in/hr-ft²-°F
@Temperature 401 - 401 °F
Average value: 0.159 W/m-K Grade Count:1
Melting Point 33.0 - 140 °C91.4 - 284 °FAverage value: 71.8 °C Grade Count:38
Crystallization Temperature 17.0 - 78.0 °C62.6 - 172 °FAverage value: 40.7 °C Grade Count:7
Maximum Service Temperature, Air 65.6 - 135 °C150 - 275 °FAverage value: 114 °C Grade Count:130
Deflection Temperature at 0.46 MPa (66 psi) 47.0 - 148 °C117 - 298 °FAverage value: 81.4 °C Grade Count:15
Deflection Temperature at 1.8 MPa (264 psi) 39.0 - 60.0 °C102 - 140 °FAverage value: 45.1 °C Grade Count:4
Vicat Softening Point 38.0 - 93.0 °C100 - 199 °FAverage value: 56.3 °C Grade Count:28
Minimum Service Temperature, Air -50.0 - -40.0 °C-58.0 - -40.0 °FAverage value: -49.2 °C Grade Count:102
Brittleness Temperature -100 - -20.0 °C-148 - -4.00 °FAverage value: -61.3 °C Grade Count:151
Glass Transition Temp, Tg -64.0 - 7.00 °C-83.2 - 44.6 °FAverage value: -38.7 °C Grade Count:43
UL RTI, Electrical 50.0 - 100 °C122 - 212 °FAverage value: 85.0 °C Grade Count:6
UL RTI, Mechanical with Impact 50.0 - 90.0 °C122 - 194 °FAverage value: 82.5 °C Grade Count:6
Clash Berg Stiffness Temperature -61.1 - 4.00 °C-78.0 - 39.2 °FAverage value: -26.9 °C Grade Count:28
Flammability, UL94 HB - V-0HB - V-0Grade Count:72
Flame Spread 18.3 - 767 mm/min0.720 - 30.2 in/minAverage value: 177 mm/min Grade Count:10
Oxygen Index 18.0 - 26.0 %18.0 - 26.0 %Average value: 22.5 % Grade Count:12
 
Optical PropertiesMetricEnglishComments
Haze 0.400 - 77.0 %0.400 - 77.0 %Average value: 27.8 % Grade Count:22
Transmission, Visible 80.0 - 90.0 %80.0 - 90.0 %Average value: 88.0 % Grade Count:14
 
Processing PropertiesMetricEnglishComments
Processing Temperature 127 - 240 °C260 - 464 °FAverage value: 192 °C Grade Count:211
Nozzle Temperature 149 - 235 °C300 - 455 °FAverage value: 204 °C Grade Count:27
Die Temperature 160 - 260 °C320 - 500 °FAverage value: 193 °C Grade Count:28
Melt Temperature 138 - 250 °C280 - 482 °FAverage value: 190 °C Grade Count:70
Mold Temperature -1.11 - 113 °C30.0 - 235 °FAverage value: 39.7 °C Grade Count:57
Drying Temperature 50.0 - 100 °C122 - 212 °FAverage value: 78.7 °C Grade Count:89
Injection Pressure 1.38 - 6.89 MPa200 - 1000 psiAverage value: 4.30 MPa Grade Count:38
Cycle Time - Injection 1.00 - 80.0 sec1.00 - 80.0 secAverage value: 38.0 sec Grade Count:27
Cushion 0.317 - 2.54 cm0.125 - 1.00 inAverage value: 1.26 cm Grade Count:5

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Polyester Thermoplastic Elastomer
Advanced Elastomer Systems Santoprene® 101-64 W175 Thermoplastic Rubber
Overview of materials for Styrenic Elastomer (TES)
Overview of materials for Silicone Rubber
Overview of materials for Thermoplastic Olefinic Elastomer (TPO)

O5440 / 78508

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.