MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow SPECFLEX™ NC 606 Polyol
Categories: Polymer

Material Notes: SPECFLEX™ NC 606 polyol is a co-polymer polyol especially designed for the production of High Resilience (HR) molded flexible foams. It processes well on all types of foam machinery. CAS# 009082-00-2 057913-80-1

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.043 g/cc1.043 g/cc
Solids Content 25.9 - 27.1 %25.9 - 27.1 %40°C; DOWM 101688-TE97A
Viscosity 1900 - 2900 cP1900 - 2900 cPCone & Plate; ISO 3219 (93)
Maximum Moisture Content 0.0700.070wt% water; ASTM D203
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 180 °C>= 356 °FASTM D93
 
Descriptive Properties
Hydroxyl Number mg KOH/g24.1 - 28.2ASTM D4274

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow VORANOL™ 4701C Polyether Polyol
Dow VORANOL™ 4703 Polyether Polyol
Dow SPECFLEX™ NC 632 Polyol
Dow VORANATE™ T-80 toluene diisocyanate (TDI)
Dow VORANOL™ 4240 Polyether Polyol

PDOW1423 / 30641

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.