MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Americas Styrenics STYRON™ 487 High-Impact Polystyrene Resin
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: STYRON™ 487 is a high-impact polystyrene with an excellent balance of flow, toughness, stiffness and heat resistance. It has excellent deep draw characteristics and is appropriate for extrusion applications where stiffness and toughness combined with high contact clarity and trim-ability are important. STYRON™ 487 can also be used in injection molding situations.

Main Characteristics
  • Heat resistance
  • Toughness
  • Stiffness
  • Complies with U.S. FDA 21 CFR 177.1640


Applications
  • Packaging/Disposables
  • Appliances
  • Housewares
  • Extrusion
  • Thermoforming
  • Injection Molding

Information provided by Dow

Americas Styrenics was formed in 2008 as a joint venture between Dow Chemical and Chevron Phillips Chemical Company. Styron was a Dow trade name before the JV formation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.04 g/cc1.04 g/ccASTM D792
Linear Mold Shrinkage 0.0030 - 0.0070 cm/cm0.0030 - 0.0070 in/inASTM D955
Melt Flow 3.2 g/10 min
@Load 5.00 kg,
Temperature 200 °C
3.2 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9797ASTM D785
Tensile Strength, Ultimate 25.5 MPa3700 psi0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638
Tensile Strength, Yield 25.9 MPa3750 psi0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638
Elongation at Break 70 %70 %0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638
Tensile Modulus 1.96 GPa284 ksi0.5 x 0.125 in. specimen; 0.2 in/min; ASTM D638
Flexural Strength 46.9 MPa6800 psi0.05 in/min; 3-point; ASTM D790
Flexural Modulus 2.28 GPa331 ksi0.05 in/min; 3-point; ASTM D790
Izod Impact, Notched  0.854 J/cm
@Thickness 3.17 mm,
Temperature -18.0 °C
1.60 ft-lb/in
@Thickness 0.125 in,
Temperature -0.400 °F
0.5 x 0.125 in.; ASTM D256
 1.76 J/cm
@Thickness 3.17 mm,
Temperature 23.0 °C
3.30 ft-lb/in
@Thickness 0.125 in,
Temperature 73.4 °F
0.5 x 0.125 in.; ASTM D256
Gardner Impact 28.2 J
@Temperature 23.0 °C
20.8 ft-lb
@Temperature 73.4 °F
ASTM D3029
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 88.9 °C192 °Funannealed; injection molded; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 75.6 °C168 °Funannealed; injection molded; ASTM D648
Vicat Softening Point 105 °C221 °F120°C/hr, 1 kg; ASTM D1525-B
Flammability, UL94 HB
@Thickness 1.52 mm
HB
@Thickness 0.0600 in
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total Lacqrene® 4241 High Impact Polystyrene
Chi Mei Polyrex® PH-888H Polystyrene - High Impact
Americas Styrenics EA6740 High Impact Polystyrene
Americas Styrenics Styron® 425 High Impact Polystyrene
Chevron Phillips EB6025 HIPS - High Impact Polystyrene

PDOW1077 / 30281

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.