MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUPOY HP5004A PC/ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Polycarbonate/ABS Alloy, Unreinforced; Polycarbonate (PC)

Material Notes: Description: Injection Molding, PC/ABS, General Purpose, Good Weld Properties, High Impact (at Low Temperature), Heat Resistance

Application: Mobile Phone Housing

CAS: 103598-77-2, 9003-56-9 and 181028-79-5

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.14 g/cc1.14 g/ccASTM D792
Maximum Moisture Content 0.0200.020Injection Molding
Linear Mold Shrinkage, Flow 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
0.0040 - 0.0060 in/in
@Thickness 0.126 in
ASTM D955
Melt Flow 5.0 g/10 min
@Load 2.16 kg,
Temperature 250 °C
5.0 g/10 min
@Load 4.76 lb,
Temperature 482 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 111111ASTM D785
Tensile Strength, Yield 54.9 MPa
@Thickness 3.20 mm
7970 psi
@Thickness 0.126 in
50mm/min; ASTM D638
Elongation at Break 100 %
@Thickness 3.20 mm
100 %
@Thickness 0.126 in
50mm/min; ASTM D638
Flexural Yield Strength 88.3 MPa
@Thickness 3.20 mm
12800 psi
@Thickness 0.126 in
10mm/min; ASTM D790
Flexural Modulus 2.26 GPa
@Thickness 3.20 mm
327 ksi
@Thickness 0.126 in
10mm/min; ASTM D790
Izod Impact, Notched  >= 4.90 J/cm
@Thickness 3.20 mm,
Temperature -30.0 °C
>= 9.18 ft-lb/in
@Thickness 0.126 in,
Temperature -22.0 °F
ASTM D256
 >= 5.88 J/cm
@Thickness 3.20 mm,
Temperature 23.0 °C
>= 11.0 ft-lb/in
@Thickness 0.126 in,
Temperature 73.4 °F
ASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 112 °C
@Thickness 6.40 mm
234 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical 60.0 °C
@Thickness >=0.750 mm
140 °F
@Thickness >=0.0295 in
UL RTI, Mechanical with Impact 60.0 °C
@Thickness >=0.750 mm
140 °F
@Thickness >=0.0295 in
UL RTI, Mechanical without Impact 60.0 °C
@Thickness >=0.750 mm
140 °F
@Thickness >=0.0295 in
Flammability, UL94 HB
@Thickness >=0.750 mm
HB
@Thickness >=0.0295 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 240 - 250 °C464 - 482 °FInjection Molding
Middle Barrel Temperature 250 - 280 °C482 - 536 °FInjection Molding
Front Barrel Temperature 250 - 280 °C482 - 536 °FInjection Molding
Nozzle Temperature 250 - 280 °C482 - 536 °FInjection Molding
Melt Temperature 255 - 285 °C491 - 545 °FInjection Molding
Mold Temperature 80.0 - 100 °C176 - 212 °FInjection Molding
Drying Temperature 80.0 - 100 °C176 - 212 °FInjection Molding
Dry Time 3.00 - 5.00 hour3.00 - 5.00 hourInjection Molding
Back Pressure 0.981 - 3.92 MPa142 - 569 psiInjection Molding
Screw Speed 40 - 70 rpm40 - 70 rpmInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Samyang Trirex® 3020IR Polycarbonate with Heat Stabilizer
LG Chemical LUPOY SC2202 PC+GF20%, High Impact
LG Chemical LUPOY EC5000A PC/ABS
Mitsubishi Xantar® LDS 3760 Polycarbonate
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

PLAY570 / 148580

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.