MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LG Chemical LUMID GP2200A(W) PA6+GF20%, General Purpose
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 20% Glass Fiber Filled

Material Notes: Feature: Injection Molding, PA6+MF23%, High ImpactPA6+GF20%, General Purpose

Application: HMID, SLMP B, Holder

CAS No. 32131-17-2 and 65997-17-3

Information provided by LG Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/ccASTM D792
Water Absorption 1.2 %1.2 %ASTM D570
Linear Mold Shrinkage, Flow 0.0060 - 0.010 cm/cm
@Thickness 3.20 mm
0.0060 - 0.010 in/in
@Thickness 0.126 in
ASTM D955
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 121121ASTM D785
Tensile Strength, Yield 147 MPa
@Thickness 3.20 mm
21300 psi
@Thickness 0.126 in
5mm/min; ASTM D638
Elongation at Break 4.0 %
@Thickness 3.20 mm
4.0 %
@Thickness 0.126 in
5mm/min; ASTM D638
Flexural Yield Strength 216 MPa
@Thickness 6.40 mm
31300 psi
@Thickness 0.252 in
3mm/min; ASTM D790
Flexural Modulus 6.67 GPa
@Thickness 6.40 mm
967 ksi
@Thickness 0.252 in
3mm/min; ASTM D790
Izod Impact, Notched 0.883 J/cm
@Thickness 6.40 mm,
Temperature 23.0 °C
1.65 ft-lb/in
@Thickness 0.252 in,
Temperature 73.4 °F
ASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmASTM D257
Dielectric Constant 3.8
@Frequency 1e+6 Hz
3.8
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 20.0 kV/mm
@Thickness 1.00 mm
508 kV/in
@Thickness 0.0394 in
ASTM D149
Arc Resistance 150 sec150 secASTM D495
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=0.750 mm
15 - 30 sec
@Thickness >=0.0295 in
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness 0.750 mm
>= 120 arcs
@Thickness 0.0295 in
High Voltage Arc-Tracking Rate, HVTR 25.4 - 50.0 mm/min1.00 - 1.97 in/min
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 45.0 µm/m-°C25.0 µin/in-°FASTM D696
Melting Point 220 °C428 °FASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 205 °C
@Thickness 6.40 mm
401 °F
@Thickness 0.252 in
Unannealed; ASTM D648
UL RTI, Electrical 65.0 °C
@Thickness >=0.750 mm
149 °F
@Thickness >=0.0295 in
UL RTI, Mechanical with Impact 65.0 °C
@Thickness >=0.750 mm
149 °F
@Thickness >=0.0295 in
UL RTI, Mechanical without Impact 65.0 °C
@Thickness >=0.750 mm
149 °F
@Thickness >=0.0295 in
Flammability, UL94 HB
@Thickness >=0.750 mm
HB
@Thickness >=0.0295 in
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 235 - 255 °C455 - 491 °FInjection Molding
Middle Barrel Temperature 240 - 270 °C464 - 518 °FInjection Molding
Front Barrel Temperature 240 - 270 °C464 - 518 °FInjection Molding
Nozzle Temperature 250 - 280 °C482 - 536 °FInjection Molding
Melt Temperature 250 - 280 °C482 - 536 °FInjection Molding
Mold Temperature 80.0 - 100 °C176 - 212 °FInjection Molding
Drying Temperature 80.0 - 100 °C176 - 212 °FInjection Molding
Dry Time 4.00 - 5.00 hour4.00 - 5.00 hourInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical LUMID GP2200B(W) PA66+GF20%, General Purpose
LG Chemical LUMID GP1300AP PA6, Plasticized
LG Chemical LUMID GP2130A(W) PA6+GF13%, General Purpose
LG Chemical LUMID GP2251AF PA6+GF25%, Flame Retardant
LG Chemical LUMID GP2251BF PA66+GF25%, Flame Retardant

PLAY135 / 148143

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.