Double quenched and tempered: carburized at 925°C (1700°F) for 8 hrs., pot cooled, reheated to 830°C (1525°F), quenched in agitated oil, reheated to 800°C (1470°F), quenched in agitated oil, 150°C (300°F) temper. 1.5 mm case depth. |
SAE J404, SAE J412, SAE J797, UNS G46200, AMS 6294, ASTM A322, ASTM A331, ASTM A505, ASTM A535, MIL SPEC MIL-S-7493 (A4620) |