MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Fujipoly Industries Sarcon® 25G-Td Thin-Film GR-TD
Categories: Polymer; Film; Thermoset; Silicone

Material Notes: Sarcon 25G-Td is a highly conformable, thermally conductive material in areas where space between surfaces is uneven and surface textures vary.

Information provided by Fujipoly Industries

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.51 g/cc2.51 g/cc70°C for 1,000 hrs; JIS-K-6220
 2.52 g/cc2.52 g/cc60°C for 1,000 hrs with 90% RH; JIS-K-6220
 2.56 g/cc2.56 g/cc50°C for 1,000 hrs; JIS-K-6220
 2.60 g/cc2.60 g/ccJIS-K-6220; ASTM D-792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4949ASTM D2240
Tensile Strength, Yield 5.00 MPa725 psi150°C for 1,000 hrs; JIS-K-6251
 6.00 MPa870 psi70°C for 1,000 hrs; JIS-K-6251
 7.00 MPa1020 psi60°C for 1,000 hrs with 90% RH; JIS-K-6251
 11.0 MPa1600 psiJIS-K-6251(#2)/ASTM D-412
Elongation at Yield 15 %15 %JIS-K-6251(#2)/ASTM D-412
 15 %15 %70°C for 1,000 hrs; JIS-K-6251
Tear Strength 11.0 kN/m62.8 pli70°C for 1,000 hrs; JIS-K-6252
 21.0 kN/m120 pliJIS-K-6252 (Angle)/ASTM D-624
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.90e+13 ohm-cm2.90e+13 ohm-cm
 7.80e+13 ohm-cm7.80e+13 ohm-cm70°C for 1,000 hrs; JIS-K-6249
 1.50e+14 ohm-cm1.50e+14 ohm-cm150°C for 1,000 hrs
 1.50e+14 ohm-cm1.50e+14 ohm-cm60°C for 1,000 hrs with 90% RH
Dielectric Strength 5.00 kV/mm127 kV/inJIS-K-6249/ASTM D-149
Dielectric Breakdown 3000 V3000 VWithstand Voltage [V/min]; JIS-K-6249/ASTM D-149
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 1.50 W/m-K10.4 BTU-in/hr-ft²-°F150°C for 1,000 hrs; JIS-R-2618
 1.50 W/m-K10.4 BTU-in/hr-ft²-°F60°C for 1,000 hrs with 90% RH; JIS-R-2618
 1.50 W/m-K10.4 BTU-in/hr-ft²-°F70°C for 1,000 hrs; JIS-R-2618
Maximum Service Temperature, Air 150 °C302 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Flammability, UL94 V-0V-0
 
Descriptive Properties
ColorDark Grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
NeoGraf eGRAF® HITHERM™ HT-2505 Graphite with Polymer Additive
ITW Insulcast® RTVS 3-95-1 Silicone Potting/Encapsulation Compound
ITW Insulcast® RTVS 27 HTC Silicone Potting/Encapsulation Compound
Fujipoly Industries Sarcon® 45Q Thin-Film QR
Dow Sylgard® 3-6605 Thermally Conductive Silicone Elastomer

PFUJIP28 / 39161

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.