MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Commercial Fine Gold, Cast
Categories: Metal; Nonferrous Metal; Precious Metal; Gold Alloy; Pure Element

Material Notes: Usual purity is 99.95-99.98%. Called proof gold if over 99.99% pure.

Key Words: Gold, Au
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 19.32 g/cc0.6980 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 3333
Tensile Strength, Ultimate 125 MPa18100 psi
Elongation at Break 30 %30 %
Modulus of Elasticity 74.5 GPa10800 ksi
Poissons Ratio 0.420.42
Fatigue Strength 31.7 MPa
@# of Cycles 1.00e+7
4600 psi
@# of Cycles 1.00e+7
reverse bend
Shear Modulus 26.2 GPa3800 ksiCalculated
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000235 ohm-cm0.00000235 ohm-cm
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 66.2 J/g28.5 BTU/lb
CTE, linear  14.2 µm/m-°C
@Temperature 20.0 °C
7.89 µin/in-°F
@Temperature 68.0 °F
 14.6 µm/m-°C
@Temperature 250 °C
8.11 µin/in-°F
@Temperature 482 °F
 15.2 µm/m-°C
@Temperature 500 °C
8.44 µin/in-°F
@Temperature 932 °F
 16.7 µm/m-°C
@Temperature 950 °C
9.28 µin/in-°F
@Temperature 1740 °F
Specific Heat Capacity 0.130 J/g-°C0.0311 BTU/lb-°F
Thermal Conductivity 300 W/m-K
@Temperature 0.000 °C
2080 BTU-in/hr-ft²-°F
@Temperature 32.0 °F
Melting Point 1064 °C1947 °F
 
Optical PropertiesMetricEnglishComments
Emissivity (0-1) 0.040
@Temperature 100 °C
0.040
@Temperature 212 °F
total spectrum
Reflection Coefficient, Visible (0-1) 0.850.85600 nm
 
Processing PropertiesMetricEnglishComments
Casting Temperature 1095 - 1300 °C2003 - 2370 °F
 
Component Elements PropertiesMetricEnglishComments
Gold, Au >= 99.95 %>= 99.95 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Gold, Au
Gold, Au; 18K, White Composition Spec (UNS P00275)
Overview of materials for Gold Alloy
Commercial Fine Gold, Wrought then Annealed
Platinum, Pt, CP Grade, Annealed

MPAu00 / 12539

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.