MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

G-9 Fiberglass Melamine Laminate Sheet
Categories: Polymer; Thermoset; Filled/Reinforced Thermoset; Melamine

Material Notes: This material is very hard, flame resistant, and has excellent electrical properties. G-9 has high arc and heat resistance and is recommended for humid environments. It is used for switch board panels, arc barriers, circuit breaker parts, and structural electrical parts. G-9 and similar fiberglass reinforced thermosets are sometimes known as garolite.

Information provide by Boedeker Plastics.

Key Words: G9 Fiber Reinforced Composite
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.85 g/cc0.0668 lb/in³ASTM D792
Water Absorption 0.60 %0.60 %24 hrs.; ASTM D570
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 115115ASTM D785
Tensile Strength at Break 352 MPa51100 psiCrosswise; ASTM D638
 425 MPa61600 psiLengthwise; ASTM D638
Flexural Strength 352 MPa51100 psiCrosswise; ASTM D790
 425 MPa61600 psiLengthwise; ASTM D790
Flexural Modulus 11.7 GPa1700 ksiCrosswise; ASTM D790
 13.8 GPa2000 ksiLengthwise; ASTM D790
Compressive Strength 448 MPa65000 psiASTM D695
Izod Impact, Notched 4.54 J/cm8.50 ft-lb/inCrosswise; ASTM D256
 6.67 J/cm12.5 ft-lb/inLengthwise; ASTM D256
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 6.3
@Frequency 1e+6 Hz
6.3
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 11.8 kV/mm300 kV/inShort Time; 1/8 inch; ASTM D149
Dissipation Factor 0.019
@Frequency 1e+6 Hz
0.019
@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 180 sec180 secASTM D495
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.9 µm/m-°C
@Temperature 20.0 °C
8.30 µin/in-°F
@Temperature 68.0 °F
Lengthwise; ASTM D696
CTE, linear, Transverse to Flow 18.0 µm/m-°C
@Temperature 20.0 °C
10.0 µin/in-°F
@Temperature 68.0 °F
Crosswise; ASTM D696
Thermal Conductivity 0.288 W/m-K2.00 BTU-in/hr-ft²-°FASTM C177
Maximum Service Temperature, Air 140 °C284 °F
Flammability, UL94 V-0V-0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
G-10 Fiberglass Epoxy Laminate Sheet
G-11 Fiberglass Epoxy Laminate Sheet
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Ensinger Tecapeek® GF30 Polyetheretherketone, 30% Glass Reinforced (PEEK)
Ensinger TECAPEI® 30% Glass Reinforced, made from Ultem® 2300 PEI

PGLAM03 / 41888

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.