MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

INEOS Styrolution PS 168 N/L GPPS
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Heat Resistant Grade

Material Notes: Styrolution PS 168N/L is a high molecular weight, heat resistant grade with high mechanical strength. It is suitable for physically or chemically expanded extruded sheet. It is also suitable for use as blend component with high impact polystyrene or Styrolux.
  • High molecular weight
  • High heat resistance
  • High mechanical strength
  • UL 94 HB (Antwerp only)

Information provided by Styrolution

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³ISO 1183
Moisture Absorption at Equilibrium <= 0.10 %
@Temperature 23.0 °C
<= 0.10 %
@Temperature 73.4 °F
50% RH; ISO 62
Water Absorption at Saturation <= 0.10 %
@Temperature 23.0 °C
<= 0.10 %
@Temperature 73.4 °F
ISO 62
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm0.0030 - 0.0060 in/inISO 294-4
Melt Flow 1.5 g/10 min
@Load 5.00 kg,
Temperature 200 °C
1.5 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 150 MPa21800 psiISO 2039-1
Tensile Strength, Yield 59.0 MPa8560 psiISO 527
Elongation at Break 3.0 %3.0 %ISO 527
Tensile Modulus 3.30 GPa479 ksiISO 527
Flexural Strength 106 MPa15400 psiISO 178
Charpy Impact Unnotched <= 2.50 J/cm²<= 11.9 ft-lb/in²ISO 179
Tensile Creep Modulus, 1 hour 3300 MPa479000 psiISO 899
Tensile Creep Modulus, 1000 hours 2600 MPa377000 psiISO 899
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+18 ohm-cm>= 1.00e+18 ohm-cmIEC 60093
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmIEC 60093
Dielectric Constant 2.5
@Frequency 100 Hz
2.5
@Frequency 100 Hz
IEC 60250
Dissipation Factor  0.000050
@Frequency 1e+6 Hz
0.000050
@Frequency 1e+6 Hz
IEC 60250
 0.000090
@Frequency 100 Hz
0.000090
@Frequency 100 Hz
IEC 60250
 
Thermal PropertiesMetricEnglishComments
CTE, linear 80.0 µm/m-°C44.4 µin/in-°FISO 11359
Thermal Conductivity 0.170 W/m-K1.18 BTU-in/hr-ft²-°FDIN 52612-1
Deflection Temperature at 0.46 MPa (66 psi) 98.0 °C208 °FISO 75
Deflection Temperature at 1.8 MPa (264 psi) 86.0 °C187 °FISO 75
Vicat Softening Point  101 °C
@Load 5.10 kg
214 °F
@Load 11.2 lb
120°C/h; ASTM D 1525
 108 °C
@Load 1.02 kg
226 °F
@Load 2.25 lb
120°C/h; ASTM D 1525
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Melt Temperature 180 - 280 °C356 - 536 °FISO 294
Mold Temperature 40.0 °C104 °FISO 294
Injection Velocity 200 mm/sec7.87 in/secISO 294

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
INEOS Styrolution PS 168N GPPS
INEOS Styrolution Polystyrol 143 E GR 2 PS
INEOS Styrolution Polystyrol 143 E GR 21 PS
LG Chemical GPPS 15NF(I) PS, High Transparency, Heat Resistance
BASF Polystyrol® 143 EO Polystyrene (Europe)

PBASG0572B / 159600

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.