MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Celanese FORTRON 214 PPS, Unfilled
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS)

Material Notes: 0214 is an unfilled grade exhibiting good melt strength. This grade demonstrates excellent heat and chemical resistance. It can be extruded to produce multi-filaments. Due to the excellent balance of flow and melt strength, this product is occasionally used for injection molding parts. Available standard in powder (0214B1), pellet (0214P1) and crystallized pellet (0214C1) form.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.35 g/cc1.35 g/ccASTM D792
Density 1.35 g/cc0.0488 lb/in³ISO 1183
Density of Compound 1.15 g/cc0.0415 lb/in³
Water Absorption 0.030 %
@Temperature 22.8 °C
0.030 %
@Temperature 73.0 °F
24hr immersion; ASTM D570
Water Absorption at Saturation 0.020 %0.020 %ISO 62
Viscosity 120000 cP120000 cP
Linear Mold Shrinkage, Flow 0.012 cm/cm0.012 in/inASTM D955
 0.012 - 0.015 cm/cm0.012 - 0.015 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.010 cm/cm0.010 in/inASTM D955
 0.015 - 0.018 cm/cm0.015 - 0.018 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9393ASTM D785
 9595ISO 2039-2
Tensile Strength at Break 86.2 MPa12500 psiASTM D638
 90.0 MPa13100 psi5mm/min; ISO 527-2/1A
Elongation at Break 3.0 %3.0 %5mm/min; ISO 527-2/1A
 3.0 %3.0 %ASTM D638
Tensile Modulus 3.80 GPa551 ksi50mm/min; ISO 527-2/1A
Flexural Strength 125 MPa18100 psiISO 178
 145 MPa21000 psiASTM D790
Flexural Modulus 3.75 GPa544 ksiISO 178
 4.14 GPa600 ksiASTM D790
Izod Impact, Notched 0.267 J/cm0.500 ft-lb/inASTM D256
Izod Impact, Unnotched 6.19 J/cm11.6 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 3.50 kJ/m²1.67 ft-lb/in²ISO 180/1A
 45.0 kJ/m²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Coefficient of Friction, Dynamic 0.140.14
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+11 ohm-cm1.00e+11 ohm-cmIEC 60093
 1.00e+16 ohm-cm1.00e+16 ohm-cmASTM D257
Dielectric Constant  3.0
@Frequency 1000 Hz
3.0
@Frequency 1000 Hz
ASTM D150
 3.0
@Frequency 1e+6 Hz
3.0
@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 17.7 kV/mm450 kV/inshort term; ASTM D149
 18.0 kV/mm457 kV/inIEC 60243-1
Dissipation Factor  0.00090
@Frequency 1e+6 Hz
0.00090
@Frequency 1e+6 Hz
ASTM D150
 0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
ASTM D150
Arc Resistance 124 sec124 secASTM D495
Comparative Tracking Index 125 V125 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 52.0 µm/m-°C28.9 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 53.0 µm/m-°C29.4 µin/in-°FISO 11359-2
Specific Heat Capacity 1.83 J/g-°C0.437 BTU/lb-°F
Thermal Conductivity 3.46 W/m-K24.0 BTU-in/hr-ft²-°FASTM C177
Melting Point 280 °C536 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 0.46 MPa (66 psi) 204 °C400 °FASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 104 °C220 °FASTM D648
 110 °C230 °FISO 75-1, -2
Deflection Temperature at 8.0 MPa 95.0 °C203 °FISO 75-1, -2
Glass Transition Temp, Tg 90.0 °C194 °FISO 11357-1,-2,-3
 
Processing PropertiesMetricEnglishComments
Processing Temperature 140 - 160 °C284 - 320 °Fcavity
 310 - 320 °C590 - 608 °Fhot runner
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Zone 1 290 - 300 °C554 - 572 °F
Zone 2 300 - 310 °C572 - 590 °F
Zone 3 310 - 320 °C590 - 608 °F
Zone 4 310 - 320 °C590 - 608 °F
Die Temperature 300 - 310 °C572 - 590 °F
Melt Temperature 295 - 330 °C563 - 626 °FISO 294
 310 - 320 °C590 - 608 °F
Mold Temperature 135 - 160 °C275 - 320 °FISO 294
Drying Temperature 110 - 120 °C230 - 248 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Moisture Content <= 0.020 %<= 0.020 %
Injection Pressure 40.0 - 80.0 MPa5800 - 11600 psi
Hold Pressure 30.0 - 60.0 MPa4350 - 8700 psi
Back Pressure <= 3.00 MPa<= 435 psi
Screw Speed  50 rpm
@Diameter 55.0 mm
50 rpm
@Diameter 2.17 in
 75 rpm
@Diameter 40.0 mm
75 rpm
@Diameter 1.57 in
 120 rpm
@Diameter 25.0 mm
120 rpm
@Diameter 0.984 in
 
Descriptive Properties
Injection moldingYes
Injection speedfast
Sheet extrusionYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese FORTRON 320 PPS, Unfilled
Celanese FORTRON 203 PPS, Unfilled
Celanese FORTRON 205 PPS, Unfilled
Celanese FORTRON 309 PPS, Unfilled
Celanese FORTRON 1140L4 PPS, 40% Glass Reinforced

PHCQ261 / 178716

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.