MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Albis Plastics POM 21 A GF10 UV Black 20% Glass Fiber  (discontinued **)
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Good Wear, Strength, Stiffness and Dimensional Stability

Applications: Gears, Housings and Engineered components

Processing: Injection Molding (Melt Temperature: 355-430°F, Mold Temperature: 190-250°F)

Data supplied by Albis Plastics Corporation.

Former ALBIS Plastics product lines have been spun off under the MOCOM brand. This specific grade was discontinued prior to the spin off.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.46 g/cc0.0527 lb/in³ASTM D792
Water Absorption 0.90 %0.90 %(24 hr); ASTM D570
Linear Mold Shrinkage 0.0080 - 0.015 cm/cm0.0080 - 0.015 in/inASTM D955
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 55.2 MPa8010 psiASTM D638
Elongation at Break 3.0 %3.0 %ASTM D638
Flexural Yield Strength 93.1 MPa13500 psiASTM D790
Flexural Modulus 3.44 GPa499 ksiASTM D790
Izod Impact, Notched 0.270 J/cm0.506 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 146 °C295 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
HB
@Thickness 0.125 in
Albis Internal Test
 
Processing PropertiesMetricEnglishComments
Melt Temperature 179 - 221 °C354 - 430 °FInjection
Mold Temperature 88.0 - 121 °C190 - 250 °F

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Asahi Kasei DELPET™ 720V Acrylic (PMMA), Standard Grade
PTS PBT-30GF 30% Glass Fiber Reinforced PBT
LG Chemical Lupox® PBT-GP-2300 30% GFR PBT
Barlog Plastics KEBAFORM C 8027 POM Copolymer, 30% mineral reinforced
Avient Edgetek® GF 5209 10 FPS 15 BLACK 30 A 1 Acetal-Copolymer, Glass Filled

PZA1A48 / 21643

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.