MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A3W Q601 PA66 (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, Unreinforced

Material Notes: Ultramid A3W Q601 is an easy flowing, heat aging resistant injection molding PA66 grade for fast processing.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc0.0408 lb/in³ISO 1183
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 85.0 MPa12300 psi50mm/min; ISO 527
Elongation at Yield 4.3 %4.3 %50mm/min; ISO 527
Tensile Modulus 3.12 GPa453 ksi1mm/min; ISO 527
Flexural Modulus 2.92 GPa424 ksiISO Data
Izod Impact, Notched (ISO) 6.00 kJ/m²2.86 ft-lb/in²ISO Test
Charpy Impact, Notched 0.600 J/cm²2.86 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Melting Point 260 °C500 °F10 K/min
 260 °C500 °FASTM Test
Deflection Temperature at 1.8 MPa (264 psi) 74.0 °C165 °FISO 75
 
Descriptive Properties
ColorNatural
Commercial StatusActive America
Impact ModifiedNo
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3K PA66 (Dry)
BASF Elastollan® C-85A Polyester Type Polyurethane Elastomer
Envalior Stanyl® TW341 PA46, Dry, Heat Stabilized
Envalior Stanyl® TW441 Nylon 46 (European and Asian Grade) (Cond)
RTP Company PermaStat® 200 Nylon 6/6 (PA), Permanently Anti-static - ESD Protection

PBASF9249 / 85013

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.