MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Menzolit Menzolit® SMC 0520 Unsaturated Polyester UP
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass SMC

Material Notes: SMC 0520 is a special SMC with significantly reduced density. The glass level has been selected to combine good moulding with sufficient strength and stiffness properties. Even without a specific fire retardant the fire retardancy level HB according the UL 94 is achieved. The product is suitable especially for applications calling for low weight and durability. Another typical application are isolating panels or mouldings that require higher strength and stiffness then standard isolating materials could provide.

Information Provided by Menzolit

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.810 g/cc0.0293 lb/in³ISO 1183
Water Absorption <= 0.50 %<= 0.50 %ISO 62
Linear Mold Shrinkage 0.00030 cm/cm0.00030 in/inISO 2577
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 13.0 MPa
@Temperature 22.0 °C
1890 psi
@Temperature 71.6 °F
25 mm flat samples, compression molded; ISO 527-4
Tensile Strength, Yield 13.0 MPa
@Temperature 22.0 °C
1890 psi
@Temperature 71.6 °F
25 mm flat samples, compression molded; ISO 527-4
Elongation at Break 0.70 %0.70 %ISO 527-4
Modulus of Elasticity 3.40 GPa493 ksi25 mm flat samples, compression molded; ISO 527-4
Flexural Strength 50.0 MPa
@Temperature 22.0 °C
7250 psi
@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Flexural Modulus 3.00 GPa
@Temperature 22.0 °C
435 ksi
@Temperature 71.6 °F
25 mm wide 100 mm long, flat samples; ISO 14125
Poissons Ratio 0.300.30
Shear Modulus 1.30 GPa189 ksiin plane
Charpy Impact, Notched 1.90 J/cm²9.04 ft-lb/in²ISO 179
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohm1.00e+12 ohmIEC 60093
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear 14.0 µm/m-°C7.78 µin/in-°FISO 11359-2
Specific Heat Capacity 1.10 J/g-°C0.263 BTU/lb-°F
Thermal Conductivity 0.700 W/m-K4.86 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 165 °C329 °F
Deflection Temperature at 1.8 MPa (264 psi) >= 200 °C>= 392 °FISO 75-2
Minimum Service Temperature, Air -40.0 °C-40.0 °F
Glass Transition Temp, Tg 170 °C338 °FISO 11357-2
Flammability, UL94 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
Oxygen Index 20 %20 %ISO 4589-2
Glow Wire Flammability Index 750 °C1380 °FIEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Processing Temperature 135 - 155 °C275 - 311 °FCompression molding, matched metal die

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Menzolit Menzolit® SMC 0412 Unsaturated Polyester UP
Menzolit Menzolit® SMC 0500 Unsaturated Polyester UP
Menzolit Menzolit® SMC 1100 Unsaturated Polyester UP
Menzolit Menzolit® SMC 1000 Unsaturated Polyester UP
Menzolit Menzolit® SMC 0420 Unsaturated Polyester UP

PMENZ046 / 100780

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.