MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Greene Tweed WR™ FP100 Polyketone, Reinforced
Categories: Polymer; Thermoplastic; Polyketone; Polyetheretherketone (PEEK)

Material Notes: Greene Tweed’s WR® FP100, a reinforced compression-molded polyketone, offers excellent wear resistance with FDA compliance. The typical properties and physical characteristics of WR FP100 make it well suited for use as bushings and wear rings in rotating equipment.

WR FP100’s FDA compliance allows it to be used in pump applications for drinking water, food processing and pharmaceutical manufacturing.

Information provided by Greene Tweed.

Vendors: Ensinger TECAPEEK™ shapes are manufactured exclusively with Victrex™ PEEK polymer. The Ensinger process and Victrex resins ensure reliability, consistency, dimensional stability, and high temperature mechanical performance.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.52 g/cc1.52 g/ccASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9797ASTM D785
Hardness, Shore D 8989ASTM D2240
Tensile Strength at Break 68.27 MPa9902 psiASTM D638
Elongation at Break 3.5 %3.5 %ASTM D1457
Flexural Strength 148.16 MPa21489 psiASTM D790
Flexural Modulus 6.44554 GPa
@Strain 0.5 %
934.847 ksi
@Strain 0.5 %
Secant; ASTM D790
Compressive Strength 222.51 MPa32272 psiASTM D695
Secant Modulus 6.15 GPa892 ksiTensile 0.5% Secant Modulus; ASTM D638
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 135 °C275 °F
Minimum Service Temperature, Air -73.3 °C-100 °F
 
Descriptive Properties
ColorTan

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Vespel® SCP-5009 Polyimide
Ensinger Tecapeek® XP-98 Compression Molded PEEK Compound, 30% Carbon Fiber
Ensinger Tecapeek® XP-98HT Compression Molded PEEK HT, 30% Carbon Fiber
Ensinger Tecapeek® XP-100 Compression Molded PEEK Compound, Bearing Grade Material with 10% Graphite, 10% PTFE, and 10% Carbon Fiber
Overview of materials for Polyetheretherketone, Carbon Fiber Filled

PGREEN71 / 42365

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.