MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

EMS-Grivory Grilamid® L 25 nat PA12 Film Grade
Categories: Polymer; Film; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12); Nylon 12, Film Grade

Material Notes: Grilamid L 25 is a high viscosity polyamide 12. This product has the following features:
  • Very tasteless
  • High toughness, even at low temperatures
  • Good resistance to weathering
  • Good chemical resistance
  • Mechanical properties only slightly dependent on relative humidity
  • Significantly lower water absorption than polyamide 6
Application examples: Grilamid L 25 is suitable for the manufacture of blown and cast film being mono or coextruded. Grilamid L 25 is used for artificial sausage casings for precooked sausages and packaging films for deep-frozen goods.

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.01 g/cc0.0365 lb/in³Dry; ISO 1183
Water Absorption 1.5 %1.5 %Sim. to ISO 62
Moisture Absorption 0.700 %0.700 %Sim. to ISO 62
Water Vapor Transmission 8.00 g/m²/day0.515 g/100 in²/day23°C/85% RH; ISO 15106-1/-2
Melt Flow 20 g/10 min20 g/10 mincm³/10min Volumetric; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 45.0 MPa6530 psiConditioned; ISO 527-1/-2
 50.0 MPa7250 psiDry; ISO 527-1/-2
Film Tensile Strength at Yield, MD 35.0 MPa5080 psiISO 527-3
Film Tensile Strength at Yield, TD 35.0 MPa5080 psiISO 527-3
Tensile Strength, Yield 40.0 MPa5800 psiConditioned; ISO 527-1/-2
 45.0 MPa6530 psiDry; ISO 527-1/-2
Film Elongation at Break, MD 850 %850 %ISO 527-3
Film Elongation at Break, TD 900 %900 %ISO 527-3
Film Elongation at Yield, MD 6.0 %6.0 %ISO 527-3
Film Elongation at Yield, TD 6.0 %6.0 %ISO 527-3
Elongation at Break >= 50 %>= 50 %Nominal, Dry; ISO 527-1/-2
 >= 50 %>= 50 %Nominal, Conditioned; ISO 527-1/-2
Elongation at Yield 10 %10 %Dry; ISO 527-1/-2
 12 %12 %Conditioned; ISO 527-1/-2
Tensile Modulus 1.10 GPa160 ksiConditioned; ISO 527-1/-2
 1.40 GPa203 ksiDry; ISO 527-1/-2
Charpy Impact Unnotched  NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Conditioned; ISO 179/1eU
 NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
Dry; ISO 179/1eU
 NB
@Temperature -30.0 °C
NB
@Temperature -22.0 °F
Dry; ISO 179/1eU
Charpy Impact, Notched  0.700 J/cm²
@Temperature -30.0 °C
3.33 ft-lb/in²
@Temperature -22.0 °F
Conditioned; ISO 179/1eA
 1.00 J/cm²
@Temperature 23.0 °C
4.76 ft-lb/in²
@Temperature 73.4 °F
Conditioned; ISO 179/1eA
Tear Strength 20.0 kN/m114 pliTrouser Tear Resistance, Parallel; ISO 6383-1
 25.0 kN/m143 pliTrouser Tear Resistance, Normal; ISO 6383-1
Film Tensile Strength at Break, MD 80.0 MPa11600 psiISO 527-3
Film Tensile Strength at Break, TD 70.0 MPa10200 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 178 °C352 °F10°C/min; ISO 11357-1/-3
Maximum Service Temperature, Air 150 °C302 °FShort Term; EMS
 
Optical PropertiesMetricEnglishComments
Gloss 150 %150 %60°; ISO 2813
 
Compliance PropertiesMetricEnglishComments
FDA YesYesFood contact
 
Descriptive Properties
Carbon Dioxide Transmission Rate, cm³/(m²*d*bar)1500ISO 15105-1/-2; 23°C/0% RH
 1600ISO 15105-1/-2; 23°C/ 85% RH
Elmendorf Tear Resistance, Normal (N)10ISO 6383-2
Elmendorf Tear Resistance, Parallel (N)10ISO 6383-2
EMS Gelboflextest [holes/m²]1300
Food contactEU Requirements
FormGranules
Gelboflextest [holes/m²], EMS1300
Industry & Consumer goodsMedical devices
MedicalUSP VI
Oxygen Transmission Rate, cm³/(m²*d*bar)350ISO 15105-1/-2; 23°C/0% RH
 370ISO 15105-1/-2; 23°C/ 85% RH
PackagingNon oriented film
ProcessingFilm Extrusion
 Injection Molding
 Other Extrusion
Product AttributesHigh viscosity

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® L 20 nat PA12
Evonik Vestamid® L2101F Nylon 12
Arkema Pebax® 7433 SA 01 MED TPA
Arkema Pebax® 7033 SA 01 MED Polyether Block Amide (PEBA)
Arkema Rilsamid® AESNO MED Nylon 12

PGRH043 / 156752

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.