MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Hostaform® C 9021 10/9005 POM, Unfilled
Categories: Polymer; Thermoplastic; Acetal (Polyoxymethylene, POM)

Material Notes: Hostaform« C 9021 10/9005 is a nominal 9 melt flow rate acetal copolymer which is capable of being permanently marked by a laser. Parts molded from Hostaform« C 9021 10/9005 can be laser marked with barcodes, identification numbers, designs, 2-D symbology, etc.

Information provided by Celanese

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.41 g/cc0.0509 lb/in³ISO 1183
Density of Compound 1.20 g/cc0.0434 lb/in³
Water Absorption at Saturation 0.65 %0.65 %ISO 62
Linear Mold Shrinkage, Flow 0.020 cm/cm0.020 in/inISO 294-4
Linear Mold Shrinkage, Transverse 0.018 cm/cm0.018 in/inISO 294-4
Melt Flow 8.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
[cm3/10min]; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 64.0 MPa9280 psi50mm/min; ISO 527-2/1A
Elongation at Break 25 %25 %
Elongation at Yield 9.0 %9.0 %50mm/min; ISO 527-2/1A
Tensile Modulus 2.85 GPa413 ksi50mm/min; ISO 527-2/1A
Flexural Modulus 2.70 GPa392 ksiISO 178
Charpy Impact Unnotched 18.0 J/cm²85.7 ft-lb/in²partial break; ISO 179/1eU
 16.0 J/cm²
@Temperature -30.0 °C
76.1 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 0.550 J/cm²2.62 ft-lb/in²ISO 179/1eA
 0.500 J/cm²
@Temperature -30.0 °C
2.38 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Tensile Creep Modulus, 1 hour 2500 MPa363000 psiISO 899-1
Tensile Creep Modulus, 1000 hours 1300 MPa189000 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant  4.0
@Frequency 1e+6 Hz
4.0
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 100 Hz
4.0
@Frequency 100 Hz
IEC 60250
Dielectric Strength 35.0 kV/mm889 kV/inIEC 60243-1
Dissipation Factor  0.0020
@Frequency 100 Hz
0.0020
@Frequency 100 Hz
IEC 60250
 0.0050
@Frequency 1e+6 Hz
0.0050
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-2
CTE, linear, Transverse to Flow 110 µm/m-°C61.1 µin/in-°FISO 11359-2
Specific Heat Capacity 2.21 J/g-°C0.528 BTU/lb-°F
Thermal Conductivity 0.155 W/m-K1.08 BTU-in/hr-ft²-°F
Melting Point 166 °C331 °F10°C/min; ISO 11357-1,-2,-3
Deflection Temperature at 1.8 MPa (264 psi) 104 °C219 °FISO 75-1, -2
Flammability, UL94  HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 - 120 °C176 - 248 °Fcavity
 190 - 210 °C374 - 410 °Fhot runner
Feed Temperature 60.0 - 80.0 °C140 - 176 °F
Zone 1 170 - 180 °C338 - 356 °F
Zone 2 180 - 190 °C356 - 374 °F
Zone 3 190 - 200 °C374 - 392 °F
Zone 4 190 - 210 °C374 - 410 °F
Die Temperature 190 - 210 °C374 - 410 °F
Melt Temperature 190 - 210 °C374 - 410 °F
Ejection Temperature 140 °C284 °F
Drying Temperature 120 - 140 °C248 - 284 °F
Dry Time 3.00 - 4.00 hour3.00 - 4.00 hour
Moisture Content <= 0.15 %<= 0.15 %
Injection Pressure 60.0 - 120 MPa8700 - 17400 psi
Hold Pressure 60.0 - 120 MPa8700 - 17400 psi
Back Pressure <= 4.00 MPa<= 580 psi
Screw Speed  70 rpm
@Diameter 55.0 mm
70 rpm
@Diameter 2.17 in
 100 rpm
@Diameter 40.0 mm
100 rpm
@Diameter 1.57 in
 150 rpm
@Diameter 25.0 mm
150 rpm
@Diameter 0.984 in
 
Descriptive Properties
Eff. thermal diffusivity4.85E-08[m^2/s]
Injection moldingYes
Injection speedslow-medium
Processing conditions acc. ISO9988
pvT (Generic Grade reference)POM K, M-RN

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Hostaform® C 9021 10/1570 POM, Specialty
Celanese Hostaform® C 9021 GV1/10 POM, 10% Glass Reinforced
Celanese Hostaform® C 9021 POM, Unfilled
Covestro Makrolon® AL2447 Polycarbonate
Celanese Hostaform® C 9021 AS POM, Specialty

PHCQ341 / 178796

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.