MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Elastollan® 1190A10 Wire & Cable Grade Polyurethane Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Polyurethane, TP

Material Notes: As with all TPU products this grade must be dried prior to processing.

Information provided by BASF Corporation.

Key Words: TPU Rubbers
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.13 g/cc
@Thickness 2.00 mm
0.0408 lb/in³
@Thickness 0.0787 in
molded plaque, cured 20 hr at 100°C; ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 90
@Thickness 2.00 mm
90
@Thickness 0.0787 in
molded plaque, cured 20 hr at 100°C; ASTM D2240
Tensile Strength, Ultimate 55.0 MPa
@Thickness 2.00 mm
7980 psi
@Thickness 0.0787 in
molded plaque, cured 20 hr at 100°C; ASTM D412
Tensile Stress at Strain  9.00 MPa
@Strain 100 %
1310 psi
@Strain 100 %
ASTM D-412
 25.0 MPa
@Strain 300 %
3630 psi
@Strain 300 %
0.76 mm (0.030 in) extruded sheet; ASTM D-412
Elongation at Break 500 %500 %on 0.030 in extruded sheet; ASTM D-412
Flexural Modulus 0.0500 GPa
@Thickness 2.00 mm
7.25 ksi
@Thickness 0.0787 in
molded plaque, cured 20 hr at 100°C; ASTM D790
Tear Strength 58.0 kN/m
@Thickness 0.762 mm
331 pli
@Thickness 0.0300 in
Split tear strength, extruded sheet; ASTM D-1938
Graves Tear Strength 114 kN/m
@Thickness 0.762 mm
650 pli
@Thickness 0.0300 in
extruded sheet; ASTM D624
Taber Abrasion, mg/1000 Cycles 30
@Thickness 2.00 mm
30
@Thickness 0.0787 in
H-18 wheel; ASTM D-1044; molded plaque, cured 20 hr at 100°C.
Compression Set 45 %
@Temperature 70.0 °C
45 %
@Temperature 158 °F
22 hr @ 70°C; ASTM D-395; 0.080 in molded plaque after curing 20 hrs at 100°C.
 25 %
@Thickness 2.00 mm
25 %
@Thickness 0.0787 in
22 hr at 23°C; molded plaque, cured 20 hr at 100°C.; ASTM D395
Tensile Set 32 %32 %at 200% elongation per ASTM D-412 is on 0.030 in extruded sheet.
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 110 °C
@Thickness 2.00 mm
230 °F
@Thickness 0.0787 in
molded plaque, cured 20 hr at 100°C; ASTM D1525
Glass Transition Temp, Tg -35.0 °C-31.0 °FPellet sample

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Elastollan® 1190A Polyether Type Polyurethane Elastomer
BASF Elastollan® 1195A Polyether Type Polyurethane Elastomer
BASF Elastollan® 1180A10 Wire & Cable Grade Polyurethane Elastomer
BASF Elastollan® C85A10 (917) Wire & Cable Grade Polyurethane Elastomer
BASF Elastollan® 1174D Polyether Type Polyurethane Elastomer

PSF994 / 67210

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.