MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lubrizol Estane® ETE 55DS3 Thermoplastic Polyurethane, Easy-to-Extrude
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: Type: Estane® ETE 55DS3 is a 55D aromatic polyester-based thermoplastic polyurethane (TPU).

Features: Hard TPU with wide extrusion processing window and melt stability, low temperature flexibility, high transparency, excellent chemical resistance.

Uses: Extrusion: Hose and Tube, Profile. Injection molding: Various.

Available in Americas, Europe, Middle East, Africa, India and Asia

Information Provided by The Lubrizol Corporation

Key Words: TPU
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.23 g/cc1.23 g/ccASTM D792
Maximum Moisture Content 0.0200.020
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 52 - 58
@Time 5.00 sec
52 - 58
@Time 0.00139 hour
ASTM D2240
Tensile Strength 71.0 MPa10300 psiASTM D412
Elongation at Break 440 %440 %ASTM D412
100% Modulus 14.5 MPa
@Strain 100 %
2100 psi
@Strain 100 %
ASTM D412
300% Modulus 33.1 MPa
@Strain 300 %
4800 psi
@Strain 300 %
ASTM D412
Tear Strength 35.9 kN/m205 pliTrouser; ASTM D470
Graves Tear Strength 154 kN/m880 pliDie C; ASTM D624
Taber Abrasion, mg/1000 Cycles 58
@Load 1.00 kg
58
@Load 2.20 lb
H-18 wheel; ASTM D3389
 
Thermal PropertiesMetricEnglishComments
Melting Point 180 °C356 °FDSC
Glass Transition Temp, Tg -39.0 °C-38.2 °FDSC
 
Processing PropertiesMetricEnglishComments
Zone 1 199 °C390 °FExtrusion
Zone 2 204 °C399 °FExtrusion
Zone 3 204 °C399 °FExtrusion
Zone 4 210 °C410 °FExtrusion
Adapter Temperature 213 °C415 °F5, Extrusion
Die Temperature 210 °C410 °F6, Zone 1, Extrusion
 210 °C410 °FZone 2, Extrusion
Drying Temperature 104 °C219 °F
Dry Time 2.00 - 4.00 hour2.00 - 4.00 hour
Dew Point -40.0 °C-40.0 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Estane® ETE 75DT3 Thermoplastic Polyurethane, Easy-to-Extrude
Lubrizol Estane® ETE 70DT3 Thermoplastic Polyurethane, Easy-to-Extrude
3D Systems DuraForm® TPU Elastomer Thermoplastic Elastomer for SLS® Systems
Ethylene Propylene Rubber (EPM, EPDM)
Polymax® Maxelast® D6760 TPE, Extruded

PNOVEON589 / 121480

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.