MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lucite International Lucite® 30B Acrylic Bead Resin
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, High Flow, Molded

Material Notes: Lucite® 30B is usually compression molded and is a high flow methyl methacrylate copolymer.

General Lucite® Acrylic Bead Resin Information: Used in casting and embedment, compression molding, dental applications, or glass separation. End products have outstanding UV resistance, Excellent weatherability, superior abrasion resistance, excellent resistance to water, alcohol, dilute acids and bases, chemical fumes, and corrosive/oxidizing environments, high gloss and hardness, water-white color and transparency, and resistance to discoloration when heated. Lucite® resins are available as minute spherical beads, water-white only (no tints) and transparent. Thermally stable to 230°C. At higher temperatures (260°C and above), they undergo smooth depolymerization to monomers, leaving negligible ash.

Data provided by the manufacturer. Properties reported below are from test specimens machined from compression molded parts.

Key Words: PMMA; Polymethyl Methacrylate; Polymethylmethacrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.18 g/cc0.0426 lb/in³
Water Absorption 0.29 %0.29 %24h
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 7575
Tensile Strength, Ultimate 67.0 MPa9720 psi
Elongation at Break 3.0 %3.0 %23°C, 50% RH
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.491
@Wavelength 589.3 nm
1.491
@Wavelength 589.3 nm
nD
Transmission, Visible 92 %92 %Luminous Transmission at 3.18 mm (0.125 in.)

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lucite International Lucite® 6751 Acrylic Bead Resin
Lucite International Lucite® 41 Acrylic Bead Resin
Lucite International Lucite® 4F Acrylic Bead Resin
Lucite International Lucite® 4G Acrylic Bead Resin
Sumitomo Chemical Sumipex® LG2 Acrylic Resin, High Flow

PICI05 / 47972

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.