MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Poly-u-Mac Air-Comb PP8-80 Polypropylene Honeycomb Material
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Air-Comb PP8-80 is a polypropylene honeycomb material that combines lightweight, strength and resilience. It is suitable for a wide variety of sandwich core applications in marine, road/ rail transportation, industry and infrastructure. Air-Comb also possesses excellent sound damping properties. Air-Comb is available in plain, contoured, and double contoured finishes and comes standard with a non-woven veil and barrier film. Air-Comb is also available without the veil and barrier film by special order. Poly-U-Mac is able to supply Air-Comb in ready-to-use kits. Designed to be used straight out of the box. Poly-U-Mac Air-Comb kits save labor costs, speed the manufacturing process and virtually eliminate material waste.

Key Features & Benefits:

  • High strength to weight ratio
  • Excellent sound dampening properties
  • Resistance to corrosion, rot and moisture
  • Wide temperature range (-22 to 176°F)
  • Recyclable
Typical Applications:
  • Leisure & Commercial Marine: decks, bulkheads, stringers & transoms
  • Road Transportation: cabs, sleeper floors, trailer beds & walls
  • Rail Transportation: floors, driver's cabs, exterior & interior paneling
  • Industry: exhibition displays, bathtubs & shower floors
  • Infrastructure: portable buildings, claddings & interior paneling

    Information provided by Poly-u-Mac

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.0801 g/cc0.00289 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Compressive Strength 1.60 MPa232 psi
Shear Strength 0.503 MPa73.0 psi
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 80.0 °C176 °F
Minimum Service Temperature, Air -30.0 °C-22.0 °F
 
Descriptive Properties
Cell Diameter8 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
EconCore ThermHex THPP80-FN Polypropylene Honeycomb Core Sheet
EconCore ThermHex THPP60-FN Polypropylene Honeycomb Core Sheet
Hexcel® HexWeb® HRH-10/F50 - 5.0 Nonmetallic Flex-Core Honeycomb
EconCore ThermHex THPP120-FN Polypropylene Honeycomb Core Sheet

PPUMC010 / 186885

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.