MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Solvay RHODAPEX® ESB-3/A2 Surfactant
Categories: Fluid

Material Notes: Chemical Name: SODIUM ALKYL ETHOXY SULFATE

CAS: 68585-34-2

Available in: Asia Pacific, Europe, Latin America and North America

Applications: RHODAPEX© ESB-3/A2 is used in the formulation of high quality shampoos, bath products, liquid soaps, and related cosmetic products. The viscosity of these sodium lauryl ethoxy sulphate based formulations can be adjusted by the addition of inorganic salts, Rodamox OB/EBA, Miratien BET C-30, and/or Alkamide DC-212/S. The mildness of a product formulated with Rhodapex ESB-3/A2 may be improved by the inclusion of cocoamphoacetates, like Minarnol C2M-NP, or a high purity amphoteric like the Mironol Ultra series.

Information provided by Rhodia, Rhodia has been acquired by Solvay.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.04 g/cc0.0376 lb/in³
pH 6.5 - 8.06.5 - 8.010% Aqueous; RP-17601
Viscosity <= 200 cP<= 200 cPRP-17619
 
Optical PropertiesMetricEnglishComments
Transmission, Visible  >= 90 %
@Wavelength 420 nm
>= 90 %
@Wavelength 420 nm
RP-17605
 >= 97 %
@Wavelength 550 nm
>= 97 %
@Wavelength 550 nm
RP-17605
 
Descriptive Properties
AppearanceClear liquidRP-17620
Cloud point0°CRP-17616
Color<150APHA
CompositionActive25-26%, MW 382, RP-17101
 Free Oil<1.2%, RP-17303
 Sodium Chloride<0.3%, RP-17504
OdorCharacteristic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Solvay RHODAPEX® EAC-70 Surfactant
Solvay RHODAPEX® EA-2 Surfactant
Solvay RHODAPEX® EST-30/BLB Surfactant
Solvay RHODAPEX® ESC-70/AB Surfactant
Solvay RHODAPEX® ESB-70/A2 Surfactant

WRHOD383 / 137614

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.