MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Avient Elastamax™ EG-9182 Thermoplastic Elastomer (TPE)  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compounds feature unique high melt strength and shear thinning characteristics compared to conventional TPE materials for enhanced processability in extrusion applications

Information provided by PolyOne

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.878 g/cc0.878 g/ccASTM D792
Melt Flow 2.7 g/10 min
@Load 5.00 kg,
Temperature 190 °C
2.7 g/10 min
@Load 11.0 lb,
Temperature 374 °F
Procedure A; ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 787810 sec; ASTM D2240
 8383ASTM D2240
Tensile Strength, Yield 6.55 MPa950 psi510 mm/min; ASTM D412A
Tensile Stress at Strain  4.76 MPa
@Strain 100 %
690 psi
@Strain 100 %
510 mm/min; ASTM D412A
 5.24 MPa
@Strain 200 %
760 psi
@Strain 200 %
510 mm/min; ASTM D412A
 5.65 MPa
@Strain 300 %
819 psi
@Strain 300 %
510 mm/min; ASTM D412A
Elongation at Break 510 %510 %510 mm/min; ASTM D412A
Tear Strength 45.5 kN/m260 pliDie C, 510 mm/min; ASTM D624
 
Descriptive Properties
FeaturesGeneral Purpose
 Good Melt Strength
FormsPellets
Generic MaterialTPE
Generic NameThermoplastic Elastomer (TPE)
Processing MethodBlow Molding
 Extrusion
 Foam Extrusion
 Profile Extrusion
 Sheet Extrusion
Regional AvailabilityAfrica & Middle East
 Asia Pacific
 Europe
 North America
 South America
UsesAutomotive Applications
 Construction Applications
 Consumer Applications
 General Purpose
 Industrial Applications

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Avient Elastamax™ EG-9072 Thermoplastic Elastomer (TPE)
Avient Elastamax™ EG-9065 Thermoplastic Elastomer (TPE)
Avient Elastamax™ EG-9165 Thermoplastic Elastomer (TPE)
Avient Elastamax™ EG-9090 Thermoplastic Elastomer (TPE)
Avient Elastamax™ EG-9190 Thermoplastic Elastomer (TPE)

PH0POL0511 / 145080

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.