MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Rogers Corporation RT/duroid® 5880 Glass Microfiber Reinforced PTFE High Frequency Laminate
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE); Polytetrafluoroethylene (PTFE), Glass Filled, Molded

Material Notes: RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to maximize benefits of fiber reinforcement in the directions most valuable to circuit producers and in the final circuit applications.

The dielectric constant of RT/duroid laminates is uniform from panel to panel and is constant over a wide frequency range. Its low dissipation factor extends the usefulness of RT/duroid 5870 and 5880 laminates to Ku-band and above.

RT/duroid 5870 and 5880 laminates are easily cut, sheared and machined to shape. They are resistant to all solvents and reagents, hot or cold, normally used in etching printed circuits or in plating edges and holes.
Available with a range of copper cladding options.

Features:

  • Lowest electrical loss for reinforced PTFE material
  • Low moisture absorption
  • Isotropic
  • Uniform electrical properties over frequency
  • Excellent chemical resistance
  • Lead free process compatible

Typical Applications:

  • Commercial Airline Telephones
  • Microstrip and Stripline Circuits
  • Millimeter Wave Applications
  • Military Radar Systems
  • Missile Guidance Systems
  • Point to Point Digital Radio Antennas

Information provided by Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 2.20 g/cc0.0795 lb/in³ASTM D792
Moisture Absorption at Equilibrium 0.020 %
@Thickness 1.57 mm
0.020 %
@Thickness 0.0620 in
D48/50; ASTM D570
Thickness 127 - 3180 microns5.00 - 125 milRange of Thicknesses Available
Deformation 1.0 %
@Pressure 14.0 MPa,
Temperature 150 °C
1.0 %
@Pressure 2030 psi,
Temperature 302 °F
Z direction; 24 hrs; ASTM D621
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  18.0 MPa
@Temperature 100 °C
2610 psi
@Temperature 212 °F
Y direction, Condition A; ASTM D638
 20.0 MPa
@Temperature 100 °C
2900 psi
@Temperature 212 °F
X direction, Condition A; ASTM D638
 27.0 MPa
@Temperature 23.0 °C
3920 psi
@Temperature 73.4 °F
Y direction, Condition A; ASTM D638
 29.0 MPa
@Temperature 23.0 °C
4210 psi
@Temperature 73.4 °F
X direction, Condition A; ASTM D638
Elongation at Break  4.9 %
@Temperature 23.0 °C
4.9 %
@Temperature 73.4 °F
Y direction, Condition A; ASTM D638
 5.8 %
@Temperature 100 °C
5.8 %
@Temperature 212 °F
Y direction, Condition A; ASTM D638
 6.0 %
@Temperature 23.0 °C
6.0 %
@Temperature 73.4 °F
X direction, Condition A; ASTM D638
 7.2 %
@Temperature 100 °C
7.2 %
@Temperature 212 °F
X direction, Condition A; ASTM D638
Tensile Modulus  0.379 GPa
@Temperature 100 °C
55.0 ksi
@Temperature 212 °F
Y direction; ASTM D638
 0.448 GPa
@Temperature 100 °C
65.0 ksi
@Temperature 212 °F
X direction; ASTM D638
 0.862 GPa
@Temperature 23.0 °C
125 ksi
@Temperature 73.4 °F
Y direction; ASTM D638
 1.08 GPa
@Temperature 23.0 °C
156 ksi
@Temperature 73.4 °F
X direction; ASTM D638
Compressive Strength  21.0 MPa
@Strain 7.8 %,
Temperature 100 °C
3050 psi
@Strain 7.8 %,
Temperature 212 °F
Y direction, Condition A; ASTM D695
 22.0 MPa
@Strain 8.4 %,
Temperature 100 °C
3190 psi
@Strain 8.4 %,
Temperature 212 °F
X direction, Condition A; ASTM D695
 27.0 MPa
@Strain 8.5 %,
Temperature 23.0 °C
3920 psi
@Strain 8.5 %,
Temperature 73.4 °F
X direction, Condition A; ASTM D695
 29.0 MPa
@Strain 7.7 %,
Temperature 23.0 °C
4210 psi
@Strain 7.7 %,
Temperature 73.4 °F
Y direction, Condition A; ASTM D695
 43.0 MPa
@Strain 17.6 %,
Temperature 100 °C
6240 psi
@Strain 17.6 %,
Temperature 212 °F
Z direction, Condition A; ASTM D695
 52.0 MPa
@Strain 12.5 %,
Temperature 23.0 °C
7540 psi
@Strain 12.5 %,
Temperature 73.4 °F
Z direction, Condition A; ASTM D695
Compressive Modulus  0.500 GPa
@Temperature 100 °C
72.5 ksi
@Temperature 212 °F
X direction, Condition A; ASTM D695
 0.500 GPa
@Temperature 100 °C
72.5 ksi
@Temperature 212 °F
Y direction, Condition A; ASTM D695
 0.670 GPa
@Temperature 100 °C
97.2 ksi
@Temperature 212 °F
Z direction, Condition A; ASTM D695
 0.710 GPa
@Temperature 23.0 °C
103 ksi
@Temperature 73.4 °F
X direction, Condition A; ASTM D695
 0.710 GPa
@Temperature 23.0 °C
103 ksi
@Temperature 73.4 °F
Y direction, Condition A; ASTM D695
 0.940 GPa
@Temperature 23.0 °C
136 ksi
@Temperature 73.4 °F
Z direction, Condition A; ASTM D695
Peel Strength 5.47 kN/m31.2 pli1 oz EDC foil; after solder float; IPC-TM-650 2.4.8
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.00e+13 ohm-cm2.00e+13 ohm-cmZ direction; C96/35/90; ASTM D257
Surface Resistance 3.00e+13 ohm3.00e+13 ohmZ direction; C96/35/90; ASTM D257
Dielectric Constant  2.2
@Frequency 8.00e+9 - 4.00e+10 Hz
2.2
@Frequency 8.00e+9 - 4.00e+10 Hz
Design; Z direction; C24/23/50; IPC-TM-650 2.5.5.5
 2.18 - 2.24
@Frequency 1e+10 Hz
2.18 - 2.24
@Frequency 1e+10 Hz
Process; Z direction; C24/23/50; IPC-TM-650 2.5.5.5
Dissipation Factor  0.00040
@Frequency 1e+6 Hz
0.00040
@Frequency 1e+6 Hz
Z direction; C24/23/50; IPC-TM-650 2.5.5.3
 0.00090
@Frequency 1e+10 Hz
0.00090
@Frequency 1e+10 Hz
Z direction; C24/23/50; IPC-TM-650 2.5.5.5
 
Thermal PropertiesMetricEnglishComments
CTE, linear  31.0 µm/m-°C
@Temperature 0.000 - 100 °C
17.2 µin/in-°F
@Temperature 32.0 - 212 °F
X-Direction; IPC-TM-650 2.4.41
 48.0 µm/m-°C
@Temperature 0.000 - 100 °C
26.7 µin/in-°F
@Temperature 32.0 - 212 °F
Y-Direction; IPC-TM-650 2.4.41
 237 µm/m-°C
@Temperature 0.000 - 100 °C
132 µin/in-°F
@Temperature 32.0 - 212 °F
Z-Direction; IPC-TM-650 2.4.41
Specific Heat Capacity 0.960 J/g-°C0.229 BTU/lb-°Fcalculated
Thermal Conductivity 0.200 W/m-K
@Temperature 80.0 °C
1.39 BTU-in/hr-ft²-°F
@Temperature 176 °F
Z direction; ASTM C518
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °FX, Y direction; ASTM D648
Decomposition Temperature 500 °C932 °FTGA; ASTM D3850
Flammability, UL94 V-0V-0
 
Descriptive Properties
Thermal Coefficient of Dielectric Constant-125 ppm/°CIPC-TM-650 2.5.5.5; -50°C to 150°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate
Rogers Corporation RT/duroid® 5880LZ Lightweight, High Frequency PTFE Laminate
Rogers Corporation RO3003 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
Rogers Corporation RO3006 Ceramic-Filled PTFE Composite, High Frequency Circuit Material
Rogers Corporation RT/duroid® 6006 Ceramic-PTFE Composite Microwave Laminate

PROGA971 / 138411

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.