MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Norplex-Micarta NP511EM Epoxy Glass Laminate Sheet, NEMA G-11
Categories: Polymer; Thermoset; Epoxy

Material Notes: NP511EM is constructed of a woven glass fabric combined with a high temperature, easy machining epoxy resin. It has excellent mechanical strength and electrical properties at elevated temperatures. The continuous operating temperature is 190°C, in mechanical applications. This material meets NEMA G-11 and MIL-I-24768/3, Type GEB.

Information provided by Norplex-Micarta

Key Words: Glass Fiber, Epoxy, Micarta, NEMA G-11, ASTM D709 Type IV Grade G-11, MIL-I-24768/3 GEB, IEC 60893-2-EP GC 203
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.80 g/cc
@Thickness 12.7 mm
1.80 g/cc
@Thickness 0.500 in
ASTM D792
Moisture Absorption 0.100 %
@Thickness 1.57 mm
0.100 %
@Thickness 0.0620 in
ASTM D570 Condition A
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 114
@Thickness 6.35 mm
114
@Thickness 0.250 in
ASTM D785
Tensile Strength  345 MPa
@Thickness 3.17 mm
50000 psi
@Thickness 0.125 in
CrossWise; ASTM D638 Condition A
 379 MPa
@Thickness 3.17 mm
55000 psi
@Thickness 0.125 in
LengthWise; ASTM D638 Condition A
Flexural Strength  448 MPa
@Thickness 1.57 mm
65000 psi
@Thickness 0.0620 in
CrossWise; ASTM D790 Condition A
 483 MPa
@Thickness 1.57 mm
70000 psi
@Thickness 0.0620 in
LengthWise; ASTM D790 Condition A
Flexural Modulus  17.2 GPa
@Thickness 1.57 mm
2500 ksi
@Thickness 0.0620 in
CrossWise; ASTM D790 Condition A
 19.3 GPa
@Thickness 1.57 mm
2800 ksi
@Thickness 0.0620 in
LengthWise; ASTM D790 Condition A
Compressive Strength 614 MPa
@Thickness 12.7 mm
89000 psi
@Thickness 0.500 in
Flatwise; ASTM D695 Condition A
Shear Strength 165 MPa
@Thickness 1.57 mm
24000 psi
@Thickness 0.0620 in
perpendicular; ASTM D732 Condition A
Izod Impact, Unnotched  5.34 J/cm
@Thickness 12.7 mm
10.0 ft-lb/in
@Thickness 0.500 in
CrossWise; ASTM D256 Condition E-48/50
 6.94 J/cm
@Thickness 12.7 mm
13.0 ft-lb/in
@Thickness 0.500 in
LengthWise; ASTM D256 Condition E-48/50
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 5.1
@Thickness 1.57 mm,
Frequency 1e+6 Hz
5.1
@Thickness 0.0620 in,
Frequency 1e+6 Hz
ASTM D150 Condition D-24/23
Dielectric Strength  13.8 kV/mm
@Thickness 1.57 mm
350 kV/in
@Thickness 0.0620 in
ASTM D149 Condition A
 15.7 kV/mm
@Thickness 1.57 mm
400 kV/in
@Thickness 0.0620 in
ASTM D149 Condition D-48/50
Dielectric Breakdown  65000 V
@Thickness 1.57 mm
65000 V
@Thickness 0.0620 in
ASTM D149 Condition D-48/50
 70000 V
@Thickness 1.57 mm
70000 V
@Thickness 0.0620 in
ASTM D149 Condition A
Dissipation Factor 0.020
@Thickness 1.57 mm,
Frequency 1e+6 Hz
0.020
@Thickness 0.0620 in,
Frequency 1e+6 Hz
ASTM D150 Condition D-24/23
Arc Resistance 170 sec
@Thickness 3.17 mm
170 sec
@Thickness 0.125 in
ASTM D495 Conition A
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 190 °C374 °F
Transformation Temperature, Tg 185 °C
@Thickness 12.7 mm
365 °F
@Thickness 0.500 in
DMA
UL RTI, Electrical 170 °C338 °FUL Bulletin 746b
UL RTI, Mechanical with Impact 180 °C356 °FUL Bulletin 746b
Flammability, UL94 HB
@Thickness 1.57 mm
HB
@Thickness 0.0620 in
 
Descriptive Properties
Bonding Strength2300[lb]; 0.5"; ASTM D229 Condition D-48/50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Norplex-Micarta NP500A Epoxy Glass Laminate Sheet, NEMA G-10
Norplex-Micarta MC511A Epoxy Glass Laminate Sheet, NEMA G-11
Elektro-Isola G-Etronax EP 203 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Norplex-Micarta MC511AF Epoxy Glass Laminate Sheet, NEMA G-11
Norplex-Micarta NP511 Epoxy Glass Laminate Sheet, NEMA G-11

PNORPM055 / 192812

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.