MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Syensqo (Solvay Specialty Polymers) Primef® 4010 Polyphenylene Sulfide (PPS), 40% Glass Fiber Reinforcement  (discontinued **)
Categories: Polymer; Thermoplastic; Polyphenylene Sulfide (PPS); Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler

Material Notes: Primef 4010 is a 40% glass fiber reinforced polyphenylene sulfide (PPS) that offers enhanced mechanical properties. In general, PPS offers an excellent balance of properties including high temperature resistance, chemical resistance, dimensional stability and electrical characteristics. Because of its inherent flame retardancy, PPS is a good choice for high-temperature electrical and electronic applications.

Features: Flame Retardant; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Processability; Good Strength; High Flow; High Heat Resistance; Low to No Water Absorption

Uses:

Availability: Europe

Holding Time: 3 sec
Cooling Time, 2 mm: 2.5 sec

Information provide by Solvay Specialty Polymers

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.66 g/cc0.0600 lb/in³ISO 1183
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cm0.0010 - 0.0030 in/inISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 180 MPa
@Temperature 23.0 °C
26100 psi
@Temperature 73.4 °F
ISO 527-2
Elongation at Break 1.7 %
@Temperature 23.0 °C
1.7 %
@Temperature 73.4 °F
ISO 527-2
Tensile Modulus 14.0 GPa
@Temperature 23.0 °C
2030 ksi
@Temperature 73.4 °F
ISO 527-2
Flexural Strength 250 MPa
@Temperature 23.0 °C
36300 psi
@Temperature 73.4 °F
ISO 178
Flexural Modulus 14.0 GPa
@Temperature 23.0 °C
2030 ksi
@Temperature 73.4 °F
ISO 178
Izod Impact, Notched 0.850 J/cm1.59 ft-lb/inASTM D256
Izod Impact, Unnotched 4.50 J/cm8.43 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+16 ohm-cm1.00e+16 ohm-cmIEC 60093
Dielectric Constant  3.9
@Frequency 1e+6 Hz
3.9
@Frequency 1e+6 Hz
IEC 60250
 4.0
@Frequency 1000 Hz
4.0
@Frequency 1000 Hz
IEC 60250
Dielectric Strength 17.0 kV/mm432 kV/inIEC 60243-1
Dissipation Factor  0.0020
@Frequency 1000 Hz
0.0020
@Frequency 1000 Hz
IEC 60250
 0.0020
@Frequency 1e+6 Hz
0.0020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 150 V150 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.300 W/m-K2.08 BTU-in/hr-ft²-°FISO 8302
Maximum Service Temperature, Air 220 °C428 °FASTM D794
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C>= 500 °FISO 75-2/A
Flammability, UL94 V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
Oxygen Index 51 %51 %ISO 4598-2
 
Processing PropertiesMetricEnglishComments
Rear Barrel Temperature 290 - 300 °C554 - 572 °F
Middle Barrel Temperature 310 - 320 °C590 - 608 °F
Front Barrel Temperature 320 - 330 °C608 - 626 °F
Nozzle Temperature 320 - 350 °C608 - 662 °F
Melt Temperature 320 - 330 °C608 - 626 °F
Mold Temperature 150 - 160 °C302 - 320 °F
Injection Pressure 50.0 - 150 MPa7250 - 21800 psi
Hold Pressure 30.0 - 150 MPa4350 - 21800 psi
Back Pressure 0.000 - 1.00 MPa0.000 - 145 psi
Screw Speed 3.0 - 10 rpm3.0 - 10 rpm
 
Descriptive Properties
Additional PropertiesSpiral Flow Length - Internal Method: 190 mm
FormsPellets
Injection RateFast
Processing MethodInjection Molding
RoHS ComplianceRoHS Compliant

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Primef® 7002 Polyphenylene Sulfide (PPS), 65% Glass\Mineral
Overview of materials for Polyphenylene Sulfide (PPS) with 40% Glass Fiber Filler
E-Polymers SEPAZ® K140HF 40% Glass Fiber Reinforced Low Flash, High Flow PPS Resin
GEHR Plastics PPS-40GF Polyphenylene Sulfide, 40% Glass Fiber
Envalior Arnite® AV2 370 XT PET-GF35

PSOLVAY176 / 122474

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.