MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Envalior TEPEX® dynalite 102-RGUD600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes: Within the TEPEX® composite laminate, Polyamide 6 is a resin known for its toughness, stiffness, abrasion resistance, heat and chemical resistances. Roving E-Glass fibers have an excellent impact performance. This makes the composite material tough and fatigue resistant while offering excellent mechanical properties.
Typical application environments are within automotive applications, large structural parts, bumper systems, structural sporting goods applications, helmet shells.

Former Lanxess (Bond Lamiantes Division) product line is now with Envalior.'

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.80 g/cc0.0650 lb/in³
Filler Content 47 %47 %by volume
Thickness 500 microns19.7 millaminate layer thickness
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 125 MPa18100 psitransverse; ISO 527-4/5
 605 MPa87700 psilongitudinal; ISO 527-4/5
Elongation at Break 1.5 %1.5 %transverse; ISO 527-4/5
 2.1 %2.1 %longitudinal; ISO 527-4/5
Tensile Modulus 12.0 GPa1740 ksitransverse; ISO 527-4/5
 30.1 GPa4370 ksilongitudinal; ISO 527-4/5
Flexural Strength 175 MPa25400 psitransverse; ISO 178
 840 MPa122000 psilongitudinal; ISO 178
Flexural Modulus 11.0 GPa1600 ksitransverse; ISO 178
 26.5 GPa3840 ksilongitudinal; ISO 178
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 °C428 °FDSC 3146
Maximum Service Temperature, Air 120 °C
@Time 7.20e+7 sec
248 °F
@Time 20000 hour
Relative Temperature Index; IEC 216/1
Deflection Temperature at 1.8 MPa (264 psi) 215 °C419 °FISO 75-1/2
Minimum Service Temperature, Air -30.0 °C-22.0 °F
Glass Transition Temp, Tg 60.0 °C140 °FDSC 3146
 
Processing PropertiesMetricEnglishComments
Processing Temperature 240 - 260 °C464 - 500 °F
 
Descriptive Properties
ReinforcementArea weight600 g/m²
 Fabrictwill
 Fibersroving glass
 Weight Rate50% longitudinal, 20% transverse
 Yarn1200 tex longitudinal and transverse

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Envalior TEPEX® dynalite 102-RG600(x)/47% Roving Glass – PA 6 Consolidated Composite Laminate
Envalior TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate
Envalior TEPEX® dynalite 104-RG600(x)/47% Roving Glass – PP Consolidated Composite Laminate
Envalior TEPEX® dynalite 208-C200(x)/45% Carbon - TPU Consolidated Composite Laminate
Envalior TEPEX® dynalite 108-FGAL290(2)-FG290(x)/45% Filament Glass – TPU Consolidated Composite Laminate

PBONDL982 / 140565

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.