MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

LyondellBasell Astryn BB77G Polypropylene Copolymer, 15% Talc  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes:
Key Features: high melt flow, high modulus, UV-stabilized, mineral-filled polypropylene copolymer, good impact stiffness and balance, good dimensional stability, good colorability, good aesthetics, excellent processability, good weatherability

Applications: automotive interior trim components, pillar moldings, sail panels

Description: Astryn BB77G high melt flow, UV-stabilized, 15% talc-filled polypropylene copolymer has an excellent balance of properties, Designed for automotive interior trim applications, this material colors easily, processes very well and provides parts with outstanding surface appearance.

Information provided by Montell Polyolefins.

LyondellBasell is the successor company to Montell.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.00 g/cc0.0361 lb/in³ISO Method 1183
Linear Mold Shrinkage 0.011 cm/cm0.011 in/inTool, Montell
Melt Flow 30 g/10 min
@Load 2.16 kg,
Temperature 230 °C
30 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 9292ISO Method 2039-2
Hardness, Shore D 6464ISO Method 868
Tensile Strength, Yield 22.0 MPa3190 psiISO Method R527-1
Elongation at Break 20 %20 %ISO Method R527-1
Flexural Modulus 2.00 GPa290 ksiISO Method 178
Izod Impact Resistance 0.320 J/cm²
@Temperature 23.0 °C
1.52 ft-lb/in²
@Temperature 73.4 °F
ISO 180
 
Thermal PropertiesMetricEnglishComments
CTE, linear 54.0 µm/m-°C
@Temperature -30.0 - 30.0 °C
30.0 µin/in-°F
@Temperature -22.0 - 86.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 109 °C228 °FISO Method 180

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LyondellBasell Hostacom™ GP622 Polypropylene Homopolymer
LyondellBasell Hostacom™ 62F4-2C Polypropylene Homopolymer
Washington Penn PPH2TF-2B Polypropylene, 20% Talc Filled
A. Schulman Fiberfil® PP-15/T/10/20 Polypropylene Homopolymer, 22% Talc Filled
LyondellBasell Moplen HP550J Polypropylene Homopolymer

PMO381 / 53616

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.